Final Magnetic Moment5.006 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.546 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.014 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRbP(HO2)2 + LiPO3 + RbPO3 + Mn2P2O7 |
Band Gap3.356 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TePb (mp-19717) | <1 1 0> | <1 0 0> | 174.2 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 107.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 87.1 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 261.3 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 174.2 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 261.3 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 261.3 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 0> | 261.3 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 158.8 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 261.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 158.8 |
BaF2 (mp-1029) | <1 1 0> | <1 0 -1> | 114.4 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 -1> | 114.4 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 107.5 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 1> | 152.0 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 114.4 |
Au (mp-81) | <1 0 0> | <1 0 0> | 87.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 261.3 |
WS2 (mp-224) | <1 0 1> | <1 0 -1> | 228.8 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 214.8 |
C (mp-48) | <1 0 0> | <0 1 0> | 214.8 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 261.3 |
LiNbO3 (mp-3731) | <1 1 1> | <1 0 0> | 261.3 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 261.3 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 -1> | 114.4 |
LiTaO3 (mp-3666) | <1 1 1> | <1 0 0> | 261.3 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 228.8 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 261.3 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 261.3 |
MgF2 (mp-1249) | <1 0 0> | <1 0 0> | 87.1 |
GaTe (mp-542812) | <0 0 1> | <1 0 -1> | 228.8 |
GaTe (mp-542812) | <1 0 -1> | <1 0 -1> | 228.8 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 261.3 |
Al2O3 (mp-1143) | <1 0 1> | <1 0 0> | 261.3 |
Fe2O3 (mp-24972) | <1 1 1> | <1 0 0> | 261.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2P6O17 (mp-758337) | 0.7266 | 0.000 | 3 |
Ni4P4O15 (mp-585202) | 0.6970 | 0.059 | 3 |
Fe2(TeO4)3 (mvc-7929) | 0.6923 | 0.300 | 3 |
Cr4P7O24 (mp-585323) | 0.7250 | 0.080 | 3 |
Ni4P4O15 (mp-705427) | 0.6915 | 0.059 | 3 |
AlP2H5O9 (mp-721876) | 0.6333 | 0.016 | 4 |
VP3(HO5)2 (mp-540982) | 0.6016 | 0.016 | 4 |
FeP2HO7 (mp-565721) | 0.5811 | 0.163 | 4 |
Cr2P4H3O16 (mp-776748) | 0.6308 | 0.082 | 4 |
GaP3(HO5)2 (mp-24465) | 0.6065 | 0.000 | 4 |
Tl2CoP4(HO2)8 (mp-865564) | 0.5923 | 0.000 | 5 |
Rb2CoP4(HO2)8 (mp-975505) | 0.5971 | 0.000 | 5 |
K2NiP4(HO2)8 (mp-764404) | 0.5579 | 0.000 | 5 |
K2ZnP4(HO2)8 (mp-757470) | 0.5585 | 0.010 | 5 |
NaCoP2HO7 (mp-703256) | 0.6088 | 0.002 | 5 |
KLiMnP3HO10 (mp-764313) | 0.5104 | 0.047 | 6 |
CsKTeH6SO10 (mp-559375) | 0.7202 | 0.000 | 6 |
NaCoBP2H2O9 (mp-601388) | 0.6784 | 0.052 | 6 |
K2NaCa2TiSi7HO20 (mp-720410) | 0.6453 | 0.000 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Rb_sv Li_sv Mn_pv P H O |
Final Energy/Atom-6.7993 eV |
Corrected Energy-248.2535 eV
Uncorrected energy = -231.1775 eV
Composition-based energy adjustment (-0.687 eV/atom x 20.0 atoms) = -13.7400 eV
Composition-based energy adjustment (-1.668 eV/atom x 2.0 atoms) = -3.3360 eV
Corrected energy = -248.2535 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)