Final Magnetic Moment5.088 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.715 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom< 0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2VCr(P2O7)2 |
Band Gap2.134 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 264.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 264.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 330.3 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 162.4 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 162.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 264.3 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 162.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 260.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 162.4 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 264.3 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 260.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 330.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 1> | 239.6 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 97.1 |
BN (mp-984) | <1 0 0> | <1 1 1> | 194.0 |
Al (mp-134) | <1 0 0> | <1 1 0> | 162.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 260.2 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 162.4 |
SiC (mp-7631) | <0 0 1> | <0 1 -1> | 291.3 |
SiC (mp-7631) | <1 0 0> | <0 0 1> | 330.3 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 198.2 |
MgO (mp-1265) | <1 0 0> | <1 1 0> | 162.4 |
TiO2 (mp-2657) | <0 0 1> | <0 1 -1> | 194.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 330.3 |
TiO2 (mp-2657) | <1 1 1> | <0 1 -1> | 291.3 |
C (mp-66) | <1 0 0> | <1 -1 1> | 154.4 |
C (mp-66) | <1 1 0> | <0 1 -1> | 291.3 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 -1> | 291.3 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 264.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 330.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 1> | 119.8 |
SiC (mp-11714) | <0 0 1> | <0 1 -1> | 291.3 |
C (mp-48) | <0 0 1> | <0 1 -1> | 291.3 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 0> | 260.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 -1> | 291.3 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 198.2 |
ZrO2 (mp-2858) | <1 0 1> | <0 0 1> | 330.3 |
Au (mp-81) | <1 0 0> | <0 0 1> | 330.3 |
Au (mp-81) | <1 1 0> | <0 1 -1> | 97.1 |
NaCl (mp-22862) | <1 0 0> | <1 1 0> | 162.4 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 -1> | 291.3 |
ZrO2 (mp-2858) | <1 1 1> | <0 0 1> | 264.3 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 198.2 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 198.2 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 1 0> | 162.4 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 132.1 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 330.3 |
CdWO4 (mp-19387) | <1 1 1> | <0 1 0> | 260.2 |
TiO2 (mp-390) | <1 0 0> | <0 1 -1> | 291.3 |
TiO2 (mp-390) | <1 1 0> | <1 -1 1> | 154.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.4186 | 0.023 | 3 |
Co5(P3O11)2 (mp-31617) | 0.4451 | 0.034 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.3503 | 0.082 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4578 | 0.028 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.4229 | 0.038 | 3 |
LiVP2O7 (mp-18911) | 0.1242 | 0.033 | 4 |
LiMoP2O7 (mp-18987) | 0.1870 | 0.000 | 4 |
LiCrP2O7 (mp-19103) | 0.0989 | 0.000 | 4 |
LiFeP2O7 (mp-19294) | 0.1314 | 0.000 | 4 |
LiScP2O7 (mp-10517) | 0.1658 | 0.000 | 4 |
Li2VCr(P2O7)2 (mp-765058) | 0.0236 | 0.004 | 5 |
Li2VCr(P2O7)2 (mp-763864) | 0.0253 | 0.003 | 5 |
Li2VCr(P2O7)2 (mp-764289) | 0.0237 | 0.000 | 5 |
Li2VCr(P2O7)2 (mp-763868) | 0.0220 | 0.003 | 5 |
Li2VCr(P2O7)2 (mp-765056) | 0.0110 | 0.000 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5825 | 0.255 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5152 | 0.330 | 6 |
Mn4Si4SnB2(HO9)2 (mp-743890) | 0.7493 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5438 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Cr_pv P O |
Final Energy/Atom-7.2587 eV |
Corrected Energy-519.6532 eV