Final Magnetic Moment3.782 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.861 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.049 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Ti3VO8 + Li2TiO3 + LiTi2O4 + V |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 211.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 211.9 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 333.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 272.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 242.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 242.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 90.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 211.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 363.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 242.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 211.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 272.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 242.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 333.0 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 333.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 242.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 242.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 363.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 151.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 176.6 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 264.9 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 242.2 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 155.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 211.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 211.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 272.5 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 121.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 30.3 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 264.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 121.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 211.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 211.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 272.5 |
BN (mp-984) | <1 1 1> | <1 0 1> | 280.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 333.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 121.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 30.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 90.8 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 264.9 |
BN (mp-984) | <1 0 0> | <1 1 1> | 155.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 90.8 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 272.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 242.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 363.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 272.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 272.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 264.9 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 242.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 211.9 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 151.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca5Mn4O9 (mp-767184) | 0.1292 | 0.026 | 3 |
MnCd4O5 (mp-766943) | 0.1347 | 0.013 | 3 |
Mg3Mn4O7 (mp-767452) | 0.1351 | 0.041 | 3 |
LiCo3O4 (mp-771200) | 0.1127 | 0.110 | 3 |
LiCoO2 (mp-894498) | 0.0857 | 0.032 | 3 |
Li3Co2CuO6 (mp-767299) | 0.0938 | 0.089 | 4 |
Li3Fe2CuO6 (mp-773288) | 0.0867 | 0.028 | 4 |
Li4VFe3O8 (mp-765728) | 0.0907 | 0.038 | 4 |
Li4Ti3MnO8 (mp-771102) | 0.0979 | 0.086 | 4 |
Li4NbV3O8 (mp-769928) | 0.0923 | 0.092 | 4 |
VO (mp-714885) | 0.2414 | 0.025 | 2 |
KN (mp-1064647) | 0.2395 | 1.464 | 2 |
In2Se3 (mp-20830) | 0.2294 | 0.530 | 2 |
SrN (mp-1078609) | 0.2134 | 0.438 | 2 |
Sb2Te3 (mp-1080789) | 0.1914 | 0.128 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6879 | 0.005 | 5 |
Hg (mp-982872) | 0.2787 | 0.020 | 1 |
Se (mp-7755) | 0.3284 | 0.181 | 1 |
Te (mp-10654) | 0.2747 | 0.047 | 1 |
Te (mp-105) | 0.2764 | 0.047 | 1 |
P (mp-53) | 0.3572 | 0.144 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv V_pv O |
Final Energy/Atom-7.4046 eV |
Corrected Energy-125.7735 eV
-125.7735 eV = -118.4732 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 1.6820 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)