Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.233 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.032 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNaNiPO4 |
Band Gap3.166 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 1> | 172.8 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 134.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 324.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 89.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 216.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 108.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 89.8 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 216.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 288.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 56.5 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 288.6 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 144.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 134.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 216.4 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 252.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 169.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 268.1 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 180.5 |
BN (mp-984) | <0 0 1> | <1 1 1> | 242.0 |
BN (mp-984) | <1 0 1> | <0 1 0> | 180.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 1> | 288.0 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 314.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 108.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 252.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 134.6 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 242.0 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 134.1 |
TeO2 (mp-2125) | <1 1 0> | <0 1 1> | 288.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 134.6 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 230.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 1 1> | 288.0 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 1> | 72.1 |
MgO (mp-1265) | <1 0 0> | <1 0 1> | 72.1 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 230.4 |
MgO (mp-1265) | <1 1 1> | <0 1 1> | 230.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 180.5 |
C (mp-66) | <1 0 0> | <0 1 1> | 115.2 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 1> | 172.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 268.1 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 224.4 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 72.1 |
TbScO3 (mp-31119) | <0 0 1> | <0 1 0> | 180.5 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 1> | 172.8 |
TbScO3 (mp-31119) | <0 1 1> | <0 1 0> | 108.3 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 288.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 314.2 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 169.4 |
InSb (mp-20012) | <1 0 0> | <1 1 0> | 134.1 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 252.7 |
PbSe (mp-2201) | <1 1 0> | <1 0 1> | 216.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2SO4 (mp-3143) | 0.4210 | 0.004 | 3 |
Na2SO4 (mp-505274) | 0.4518 | 0.006 | 3 |
Li2SO4 (mp-558382) | 0.4109 | 0.055 | 3 |
Na2CrO4 (mp-18779) | 0.3204 | 0.000 | 3 |
Na2FeO4 (mp-19044) | 0.3239 | 0.062 | 3 |
LiCrPO4 (mp-761401) | 0.3188 | 0.077 | 4 |
NaFePO4 (mp-763946) | 0.1683 | 0.006 | 4 |
NaVSiO4 (mp-770062) | 0.2338 | 0.041 | 4 |
NaMnPO4 (mp-19619) | 0.2948 | 0.011 | 4 |
NaFePO4 (mp-19226) | 0.3171 | 0.000 | 4 |
Li7Mn7P6(O8F)3 (mp-763896) | 0.5563 | 0.022 | 5 |
Li7V7P6(O8F)3 (mp-763895) | 0.5637 | 0.131 | 5 |
Li4V2Si(PO6)2 (mp-770190) | 0.5518 | 0.258 | 5 |
SrMnV2(AgO4)2 (mp-622099) | 0.5092 | 0.028 | 5 |
SrMnV2(AgO4)2 (mp-561287) | 0.5066 | 0.028 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Na_pv Ni_pv P O |
Final Energy/Atom-6.1371 eV |
Corrected Energy-95.8662 eV
-95.8662 eV = -85.9198 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 4.3280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)