Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.578 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.24 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3VO4 + LiF |
Band Gap3.885 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 273.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 156.7 |
LaAlO3 (mp-2920) | <1 1 0> | <0 0 1> | 241.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 193.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 48.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 279.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 193.3 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 193.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 208.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 178.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 158.6 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 178.1 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 330.8 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 152.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 50.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 145.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 279.9 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 156.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 178.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 -1> | 52.9 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 52.2 |
LaAlO3 (mp-2920) | <1 1 1> | <1 0 1> | 256.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 158.6 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 178.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 -1> | 158.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 156.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 229.0 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 203.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 171.2 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 229.0 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 356.3 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 218.4 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 211.5 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 203.6 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 178.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 145.0 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 152.7 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 203.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 145.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 127.2 |
Te2W (mp-22693) | <0 1 1> | <1 1 1> | 178.6 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 330.8 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 171.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 178.1 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 313.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 208.9 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 193.3 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 85.6 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 241.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 203.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca4SnS6 (mp-866473) | 0.5991 | 0.146 | 3 |
Li5Cr2O8 (mp-763843) | 0.5772 | 0.063 | 3 |
Li3CrO4 (mp-763703) | 0.6411 | 0.058 | 3 |
Li5(CoO3)2 (mp-763696) | 0.5123 | 0.106 | 3 |
Na6Sn2O7 (mp-773498) | 0.6586 | 0.072 | 3 |
Li7VGeO8 (mp-769539) | 0.5323 | 0.019 | 4 |
Li2CrSiO4 (mp-761406) | 0.5489 | 0.339 | 4 |
Li4V(PO4)2 (mp-761335) | 0.6251 | 0.097 | 4 |
Li2Si4Ni5O14 (mp-765539) | 0.6328 | 0.071 | 4 |
Li6VO5F (mp-765511) | 0.6161 | 0.070 | 4 |
Cr3N4 (mp-1015065) | 0.7080 | 0.387 | 2 |
Sr2AlCr2GaO7 (mvc-312) | 0.7338 | 0.186 | 5 |
Sr2AlV2GaO7 (mvc-350) | 0.7442 | 0.325 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-5.9214 eV |
Corrected Energy-127.4111 eV
-127.4111 eV = -118.4288 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction) - 3.3640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)