Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.552 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.53 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2O5 + LiF |
Band Gap2.445 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 250.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 235.0 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 107.2 |
AlN (mp-661) | <1 1 0> | <1 1 -1> | 189.7 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 282.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 206.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 235.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 313.3 |
BaF2 (mp-1029) | <1 0 0> | <1 -1 0> | 322.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 219.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 188.0 |
GaN (mp-804) | <1 0 1> | <1 0 -1> | 192.7 |
GaN (mp-804) | <1 1 0> | <1 -1 -1> | 227.9 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 206.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 344.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 250.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 250.7 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 235.0 |
KCl (mp-23193) | <1 0 0> | <1 -1 0> | 322.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 -1> | 287.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 214.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 282.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 285.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 -1> | 284.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 282.0 |
InAs (mp-20305) | <1 1 0> | <1 -1 1> | 268.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 235.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 313.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 287.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 156.7 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 0> | 258.0 |
CdS (mp-672) | <0 0 1> | <0 1 -1> | 229.9 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 256.9 |
CdS (mp-672) | <1 0 1> | <0 1 -1> | 287.4 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 293.8 |
CdS (mp-672) | <1 1 1> | <1 -1 0> | 258.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 282.0 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 156.7 |
LiF (mp-1138) | <1 1 1> | <1 -1 0> | 258.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 344.6 |
Te2W (mp-22693) | <0 1 0> | <1 -1 1> | 268.8 |
Te2W (mp-22693) | <0 1 1> | <1 -1 -1> | 227.9 |
YVO4 (mp-19133) | <1 0 0> | <1 -1 0> | 193.5 |
YVO4 (mp-19133) | <1 0 1> | <1 1 -1> | 284.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 344.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 313.3 |
Te2Mo (mp-602) | <1 0 0> | <1 -1 1> | 268.8 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 321.1 |
Ag (mp-124) | <1 1 0> | <0 1 -1> | 172.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 344.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2Mn2F7 (mp-764861) | 0.6151 | 0.096 | 3 |
Li2MnF4 (mp-777718) | 0.6988 | 0.103 | 3 |
MgTi3O7 (mvc-8898) | 0.6910 | 0.115 | 3 |
V3ZnO7 (mvc-9164) | 0.6668 | 0.057 | 3 |
ZnCo3O7 (mvc-9173) | 0.6503 | 0.334 | 3 |
Zn2SbWO6 (mvc-7378) | 0.7334 | 0.240 | 4 |
ZnAs2WO7 (mvc-8251) | 0.7341 | 0.164 | 4 |
Zn2TeWO6 (mvc-6194) | 0.7280 | 0.344 | 4 |
CrN2 (mp-1016069) | 0.7292 | 0.474 | 2 |
Fe2CuAs2(HO5)2 (mp-762871) | 0.6850 | 0.103 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-6.4333 eV |
Corrected Energy-155.2835 eV
-155.2835 eV = -141.5326 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)