Final Magnetic Moment6.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.719 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3V2(PO4)3 + Li4P2O7 + LiVP2O7 |
Band Gap1.694 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 1 1> | 160.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 136.6 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 255.8 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 136.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 136.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 170.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 85.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 255.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 136.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 85.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 255.8 |
BN (mp-984) | <1 0 1> | <1 1 1> | 160.8 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 255.8 |
Al (mp-134) | <1 1 0> | <0 1 0> | 136.6 |
Al (mp-134) | <1 1 1> | <0 0 1> | 85.3 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 136.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 170.5 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 255.8 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 136.6 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 170.5 |
C (mp-66) | <1 0 0> | <0 0 1> | 255.8 |
C (mp-66) | <1 1 0> | <0 0 1> | 255.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 85.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 255.8 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 255.8 |
MoSe2 (mp-1634) | <1 0 1> | <1 1 1> | 160.8 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 255.8 |
NaCl (mp-22862) | <1 1 0> | <0 1 0> | 136.6 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 255.8 |
C (mp-48) | <1 0 1> | <1 1 1> | 160.8 |
CdWO4 (mp-19387) | <0 1 1> | <1 1 1> | 160.8 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 255.8 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 170.5 |
Ge (mp-32) | <1 1 0> | <1 1 0> | 136.7 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 255.8 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 255.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn4Si4O13 (mp-767874) | 0.7233 | 0.073 | 3 |
Cu3(P2O7)2 (mp-772942) | 0.7304 | 0.058 | 3 |
Co3(AsO4)2 (mp-690538) | 0.7060 | 0.229 | 3 |
Ni5(PO4)4 (mp-32329) | 0.7021 | 0.046 | 3 |
Fe3P3O13 (mvc-12891) | 0.7265 | 0.100 | 3 |
LiFeP2O7 (mp-850161) | 0.5698 | 0.069 | 4 |
Li5Fe4(P2O7)4 (mp-849492) | 0.5282 | 0.045 | 4 |
Li9V3P8O29 (mp-765711) | 0.4507 | 0.150 | 4 |
Li9V3P8O29 (mp-765489) | 0.1669 | 0.114 | 4 |
LiV(PO3)3 (mp-32515) | 0.5999 | 0.017 | 4 |
Li3V2P4(HO8)2 (mp-850257) | 0.6497 | 0.066 | 5 |
Li3V2P4(HO8)2 (mp-780314) | 0.6787 | 0.060 | 5 |
LiV3Fe2CuO12 (mp-767459) | 0.6226 | 0.017 | 5 |
Li3V2P4(HO8)2 (mp-777491) | 0.6695 | 0.061 | 5 |
Li3V2P4(HO8)2 (mp-781013) | 0.6562 | 0.067 | 5 |
Na3Mg4CrSi8(O11F)2 (mp-743787) | 0.5322 | 0.709 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-6.9197 eV |
Corrected Energy-728.9506 eV