Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.387 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.084 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.71 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiPO3 + Na4Mn2O5 + CO2 + C |
Band Gap3.650 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 -1> | 247.8 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 233.8 |
AlN (mp-661) | <1 0 1> | <1 1 -1> | 247.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 242.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 143.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 137.1 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 274.2 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 152.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 215.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 143.8 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 247.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 302.6 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 242.1 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 242.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 242.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 -1> | 274.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 -1> | 165.2 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 302.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 137.1 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 274.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 242.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 359.5 |
CdS (mp-672) | <0 0 1> | <1 1 -1> | 247.8 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 143.8 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 256.9 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 205.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 68.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 323.5 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 71.9 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 0> | 230.4 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 121.0 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 216.5 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 274.2 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 230.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 215.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 216.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 107.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 1> | 216.5 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 287.6 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 230.4 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 230.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 230.4 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 205.7 |
C (mp-66) | <1 0 0> | <1 0 -1> | 205.7 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 322.6 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 276.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 359.5 |
C (mp-66) | <1 1 1> | <1 0 0> | 181.6 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 230.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 215.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na3ZnPCO7 (mp-767545) | 0.3551 | 0.002 | 5 |
Na3MnAsCO7 (mp-771476) | 0.3024 | 0.115 | 5 |
Na5Mn2P2(CO7)2 (mp-770045) | 0.3366 | 0.013 | 5 |
Na5Mn2P2(CO7)2 (mp-769465) | 0.3261 | 0.002 | 5 |
Na3MnPCO7 (mp-19261) | 0.3210 | 0.000 | 5 |
Na2LiFePCO7 (mp-773678) | 0.3561 | 0.132 | 6 |
Na5LiMn2P2(CO7)2 (mp-773420) | 0.3449 | 0.082 | 6 |
Na5LiMn2P2(CO7)2 (mp-770027) | 0.3558 | 0.076 | 6 |
Na5LiMn2P2(CO7)2 (mp-773773) | 0.3373 | 0.266 | 6 |
Na5LiMn2P2(CO7)2 (mp-773680) | 0.3363 | 0.273 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv Mn_pv P C O |
Final Energy/Atom-6.7238 eV |
Corrected Energy-188.0138 eV
-188.0138 eV = -174.8201 eV (uncorrected energy) - 9.8321 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)