Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.470 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVOF3 + V2O5 |
Band Gap1.719 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 46.1 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 156.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 138.2 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 241.6 |
BaF2 (mp-1029) | <1 1 0> | <1 1 1> | 227.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 138.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 264.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 132.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 121.4 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 132.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 138.2 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 241.6 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 227.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 276.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 313.2 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 211.2 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 227.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 256.4 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 264.0 |
CdS (mp-672) | <1 1 0> | <1 1 1> | 151.6 |
LiF (mp-1138) | <1 0 0> | <1 0 -1> | 313.2 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 211.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 322.6 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 192.3 |
Te2W (mp-22693) | <1 1 0> | <1 1 1> | 227.4 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 313.2 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 184.3 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 202.3 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 192.3 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 256.4 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 158.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 237.6 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 227.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 138.2 |
CeO2 (mp-20194) | <1 0 0> | <1 0 -1> | 117.5 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 211.2 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 306.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 184.8 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 39.2 |
BN (mp-984) | <1 0 1> | <1 0 0> | 79.2 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 290.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 138.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 151.6 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 121.4 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 320.5 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 313.2 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 338.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 303.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 211.2 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 256.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-2.68452 | 0.03343 | -0.41421 | 0.00000 | -0.11054 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.61564 | 0.00000 | -0.34998 |
0.66787 | -1.47917 | -2.60503 | 0.00000 | -1.49240 | 0.00000 |
Piezoelectric Modulus ‖eij‖max3.42490 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
7.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
4.16 | 0.00 | -0.05 |
0.00 | 4.90 | 0.00 |
-0.05 | 0.00 | 7.05 |
Dielectric Tensor εij (total) |
||
---|---|---|
6.90 | 0.00 | -1.97 |
0.00 | 17.52 | 0.00 |
-1.97 | 0.00 | 73.89 |
Polycrystalline dielectric constant
εpoly∞
5.37
|
Polycrystalline dielectric constant
εpoly
32.77
|
Refractive Index n2.32 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V4O7F5 (mp-779960) | 0.4114 | 0.043 | 3 |
VO2F (mp-764057) | 0.3159 | 0.053 | 3 |
VO2F (mp-764572) | 0.3530 | 0.037 | 3 |
V4O7F5 (mp-849586) | 0.3202 | 0.063 | 3 |
VO2F (mp-778616) | 0.3919 | 0.029 | 3 |
WXeOF6 (mp-565584) | 0.7289 | 0.134 | 4 |
RbVOF3 (mp-565881) | 0.7196 | 0.000 | 4 |
MoO3 (mvc-14941) | 0.6491 | 0.010 | 2 |
MoO3 (mp-715463) | 0.5609 | 0.038 | 2 |
MoO3 (mp-715584) | 0.7448 | 0.002 | 2 |
MoO3 (mp-510584) | 0.5588 | 0.039 | 2 |
MoO3 (mp-18856) | 0.6797 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv O F |
Final Energy/Atom-6.7982 eV |
Corrected Energy-61.4578 eV
Uncorrected energy = -54.3858 eV
Composition-based energy adjustment (-0.687 eV/atom x 4.0 atoms) = -2.7480 eV
Composition-based energy adjustment (-0.462 eV/atom x 2.0 atoms) = -0.9240 eV
Composition-based energy adjustment (-1.700 eV/atom x 2.0 atoms) = -3.4000 eV
Corrected energy = -61.4578 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)