Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.230 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.093 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.90 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToY6WO12 + Y2WO6 + Li4WO5 |
Band Gap2.788 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC222 [21] |
HallC 2 2 |
Point Group222 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 64.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 106.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 318.9 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 154.8 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 282.9 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 193.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 275.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 232.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 64.4 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 322.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 141.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 1> | 220.6 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 77.4 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 106.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 64.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 141.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 64.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 70.9 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 282.9 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 283.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 283.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 283.5 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 70.9 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 177.2 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 220.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 322.2 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 106.3 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 282.9 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 354.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 193.3 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 154.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 141.7 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 77.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 322.2 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 248.1 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 283.5 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 177.2 |
Te2Mo (mp-602) | <1 1 0> | <1 0 0> | 275.3 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 154.8 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 70.9 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 177.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 257.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 206.5 |
BN (mp-984) | <1 0 0> | <0 1 0> | 283.5 |
BN (mp-984) | <1 0 1> | <1 0 1> | 282.9 |
BN (mp-984) | <1 1 0> | <0 1 1> | 294.2 |
BN (mp-984) | <1 1 1> | <1 1 0> | 309.7 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 232.3 |
Bi2Se3 (mp-541837) | <1 0 1> | <0 1 0> | 248.1 |
MoS2 (mp-1434) | <0 0 1> | <1 0 1> | 282.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.84869 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.16625 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.43401 |
Piezoelectric Modulus ‖eij‖max0.84869 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
4.22 | 0.00 | 0.00 |
0.00 | 4.32 | 0.00 |
0.00 | 0.00 | 3.89 |
Dielectric Tensor εij (total) |
||
---|---|---|
21.44 | 0.00 | 0.00 |
0.00 | 9.93 | 0.00 |
0.00 | 0.00 | 14.72 |
Polycrystalline dielectric constant
εpoly∞
4.14
|
Polycrystalline dielectric constant
εpoly
15.36
|
Refractive Index n2.04 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMn5O10 (mp-763699) | 0.6099 | 0.994 | 3 |
Co(CuO2)4 (mp-773277) | 0.5882 | 0.053 | 3 |
LiV2F5 (mp-765440) | 0.5507 | 0.064 | 3 |
Mg(SnO2)2 (mvc-6826) | 0.5917 | 0.162 | 3 |
Zn(SnO2)2 (mvc-6860) | 0.5269 | 0.149 | 3 |
Li2Mn2OF6 (mp-767010) | 0.5756 | 0.011 | 4 |
Li2Fe2OF6 (mp-777626) | 0.6196 | 0.474 | 4 |
LiV6O7F5 (mp-849986) | 0.6297 | 0.118 | 4 |
ZnCuBiO5 (mvc-8909) | 0.4969 | 0.131 | 4 |
CaCuBiO5 (mvc-9029) | 0.5342 | 0.092 | 4 |
V3O5 (mp-714914) | 0.6301 | 0.004 | 2 |
V3O5 (mp-622497) | 0.6237 | 0.004 | 2 |
V5O9 (mp-558587) | 0.6263 | 0.008 | 2 |
V7O13 (mp-715920) | 0.6325 | 0.038 | 2 |
V6O11 (mp-714930) | 0.6308 | 0.013 | 2 |
Li4MnNb2WO12 (mp-771475) | 0.6930 | 0.044 | 5 |
Li4CrTe2WO12 (mp-775509) | 0.7356 | 0.109 | 5 |
Li4CrTe(WO6)2 (mp-777147) | 0.7120 | 0.168 | 5 |
Li4MnNb(WO6)2 (mp-771868) | 0.7249 | 0.027 | 5 |
LaZnFeWO6 (mvc-9052) | 0.7320 | 0.080 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Y_sv W_pv O |
Final Energy/Atom-8.1442 eV |
Corrected Energy-115.8086 eV
Uncorrected energy = -105.8746 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-4.438 eV/atom x 1.0 atoms) = -4.4380 eV
Corrected energy = -115.8086 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)