Final Magnetic Moment3.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.689 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3VO4 + V3O5 + V2O3 + LiF |
Band Gap1.096 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 223.3 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 223.3 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 202.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 159.6 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 223.3 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 265.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 297.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 183.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 212.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 319.1 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 223.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 223.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 289.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 159.6 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 223.3 |
KCl (mp-23193) | <1 1 1> | <1 1 0> | 274.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 319.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 -1> | 214.4 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 159.6 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 223.3 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 265.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 159.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 244.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 212.8 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 319.1 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 305.6 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 223.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 305.6 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 192.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 183.3 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 1> | 289.0 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 305.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 265.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 305.6 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 223.3 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 183.3 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 183.3 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 212.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 183.3 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 101.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 122.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 -1> | 268.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 265.9 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 305.6 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 159.6 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 319.1 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 319.1 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 265.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5NbO5 (mp-770649) | 0.5553 | 0.021 | 3 |
Li5SbO5 (mp-29364) | 0.5606 | 0.000 | 3 |
Li5BiO5 (mp-29365) | 0.6167 | 0.000 | 3 |
Li5MnO5 (mp-770101) | 0.6229 | 0.063 | 3 |
Li5TaO5 (mp-755013) | 0.5722 | 0.000 | 3 |
Li3V2(O2F)2 (mp-764397) | 0.4889 | 0.064 | 4 |
Li5MnO3F2 (mp-767042) | 0.4881 | 0.054 | 4 |
Li3Cu4NiO8 (mp-770350) | 0.5296 | 0.046 | 4 |
Li5NiO3F2 (mp-764683) | 0.5280 | 0.093 | 4 |
Li5VO4F (mp-765359) | 0.5349 | 0.046 | 4 |
Fe13O15 (mp-767312) | 0.7072 | 0.601 | 2 |
Ti11O14 (mp-759754) | 0.7196 | 0.047 | 2 |
Fe3O4 (mp-715614) | 0.6719 | 0.468 | 2 |
Cr3O4 (mp-772696) | 0.6944 | 0.082 | 2 |
Y3Se4 (mp-32727) | 0.7093 | 0.013 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-6.3569 eV |
Corrected Energy-152.1974 eV
-152.1974 eV = -139.8511 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)