Final Magnetic Moment0.420 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.422 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.999 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeBO3 + Fe3BO5 + LiBO2 |
Band Gap1.823 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPc [7] |
HallP 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 142.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 237.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 189.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 277.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 237.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 277.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 189.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 332.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 284.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 215.8 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 237.2 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 277.5 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 277.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 270.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 332.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 324.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 284.6 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 270.4 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 270.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 142.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 237.2 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 214.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 284.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 332.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 142.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 270.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 270.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 216.3 |
BN (mp-984) | <1 0 0> | <0 1 1> | 215.8 |
BN (mp-984) | <1 1 0> | <0 1 0> | 162.2 |
BN (mp-984) | <1 1 1> | <1 1 1> | 236.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 237.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 332.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 270.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 47.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 284.6 |
Al (mp-134) | <1 0 0> | <1 1 0> | 214.3 |
Al (mp-134) | <1 1 0> | <0 1 0> | 270.4 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 214.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 284.6 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 277.5 |
CdTe (mp-406) | <1 0 0> | <1 1 0> | 214.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 284.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 332.0 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 237.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 277.5 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 210.6 |
BN (mp-984) | <0 0 1> | <0 0 1> | 142.3 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 324.4 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 332.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3MnF5 (mp-763332) | 0.6804 | 0.083 | 3 |
Li3BO3 (mp-27275) | 0.7012 | 0.000 | 3 |
Li6B4O9 (mp-768875) | 0.7143 | 0.063 | 3 |
Na3CoO3 (mp-777919) | 0.5444 | 0.127 | 3 |
Li6B4O9 (mp-1020024) | 0.6358 | 0.000 | 3 |
Li7Fe8(BO3)8 (mp-764896) | 0.2425 | 0.015 | 4 |
Li5Fe6(BO3)6 (mp-769427) | 0.2151 | 0.049 | 4 |
Li3Mn4(BO3)4 (mp-780136) | 0.2338 | 0.039 | 4 |
Li7Fe8(BO3)8 (mp-850450) | 0.2467 | 0.009 | 4 |
Li7Fe8(BO3)8 (mp-764523) | 0.2365 | 0.015 | 4 |
Li8MnFe7(BO3)8 (mp-850743) | 0.3599 | 0.017 | 5 |
Li4MnFe2(BO3)4 (mp-767642) | 0.3073 | 0.055 | 5 |
Li8Mn3Fe5(BO3)8 (mp-778883) | 0.3687 | 0.015 | 5 |
Li8Mn5Fe3(BO3)8 (mp-780292) | 0.3716 | 0.011 | 5 |
Li4MnFe3(BO3)4 (mp-779783) | 0.3695 | 0.016 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv B O |
Final Energy/Atom-6.0453 eV |
Corrected Energy-316.8013 eV
-316.8013 eV = -278.0824 eV (uncorrected energy) - 21.8640 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)