Final Magnetic Moment1.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.482 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.143 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa2FeO3 + Na2O2 |
Band Gap0.316 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 1 0> | <1 0 0> | 147.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 220.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 220.5 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 140.6 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 295.7 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 295.7 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 152.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 295.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 295.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 294.0 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 134.6 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 295.7 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 73.5 |
BN (mp-984) | <1 0 1> | <1 1 0> | 283.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 294.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 295.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 294.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 220.5 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 295.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 140.6 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 283.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 134.6 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 220.5 |
Al (mp-134) | <1 1 1> | <1 0 0> | 220.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 -1> | 134.6 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 283.0 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 220.5 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 295.7 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 188.7 |
BN (mp-984) | <0 0 1> | <1 1 0> | 283.0 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 295.7 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 177.4 |
BN (mp-984) | <1 0 0> | <1 0 0> | 294.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 294.0 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 236.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 294.0 |
Al (mp-134) | <1 0 0> | <0 1 0> | 295.7 |
Al (mp-134) | <1 1 0> | <1 0 0> | 294.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 295.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 140.6 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 283.0 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 283.0 |
C (mp-66) | <1 1 0> | <0 1 0> | 295.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 220.5 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 220.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 140.6 |
Mg (mp-153) | <1 0 0> | <1 0 -1> | 134.6 |
KP(HO2)2 (mp-23959) | <1 0 1> | <1 0 -1> | 134.6 |
KP(HO2)2 (mp-23959) | <1 1 0> | <1 0 -1> | 134.6 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 220.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
K4UO5 (mp-8794) | 0.4441 | 0.000 | 3 |
Na3NbO4 (mp-27247) | 0.3988 | 0.000 | 3 |
Na4WO5 (mp-19334) | 0.4964 | 0.000 | 3 |
Na4TeO5 (mp-15391) | 0.4185 | 0.000 | 3 |
Na3FeO4 (mp-778416) | 0.5176 | 0.009 | 3 |
Li2VO2F (mp-763225) | 0.6519 | 0.103 | 4 |
Li2VO2F (mp-763345) | 0.6998 | 0.238 | 4 |
KPr6OsI10 (mp-568343) | 0.7050 | 0.000 | 4 |
Ca2AgWO6 (mvc-5942) | 0.6244 | 0.086 | 4 |
Na3Cu2SbO6 (mp-12860) | 0.6842 | 0.056 | 4 |
Te2Au (mp-20123) | 0.7482 | 0.000 | 2 |
K3Na2LiTeO6 (mp-559875) | 0.7388 | 0.000 | 5 |
Ca14La6Mg3Ti17O60 (mp-695227) | 0.7401 | 0.011 | 5 |
Sr3LaMn2(WO6)2 (mp-706225) | 0.7486 | 0.031 | 5 |
LaMgFeCuO6 (mvc-8936) | 0.7360 | 0.092 | 5 |
LaZnFeCuO6 (mvc-9037) | 0.7047 | 0.292 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Na_pv Fe_pv O |
Final Energy/Atom-4.8137 eV |
Corrected Energy-176.2078 eV
-176.2078 eV = -154.0392 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)