Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.601 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + LiMn(PO3)4 + Li6V3P8O29 + VP2O7 |
Band Gap1.421 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 257.7 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 157.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 257.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 162.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 243.9 |
Bi2Se3 (mp-541837) | <1 0 0> | <0 0 1> | 243.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 -1> | 228.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 243.9 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 243.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 243.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 162.6 |
LiTaO3 (mp-3666) | <1 0 1> | <0 1 -1> | 228.8 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 243.9 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 162.6 |
Ni (mp-23) | <1 0 0> | <1 1 -1> | 171.8 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 243.9 |
SiC (mp-11714) | <1 1 0> | <0 0 1> | 162.6 |
Si (mp-149) | <1 1 1> | <1 0 0> | 257.7 |
Au (mp-81) | <1 0 0> | <0 0 1> | 243.9 |
Au (mp-81) | <1 1 0> | <0 0 1> | 243.9 |
Ga2O3 (mp-886) | <1 1 1> | <1 0 0> | 257.7 |
WS2 (mp-224) | <1 0 1> | <0 1 0> | 222.6 |
C (mp-48) | <1 0 1> | <0 1 0> | 222.6 |
ZrO2 (mp-2858) | <0 1 0> | <0 1 0> | 111.3 |
SiC (mp-8062) | <1 0 0> | <1 1 -1> | 171.8 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 162.6 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 243.9 |
CdWO4 (mp-19387) | <0 1 1> | <0 0 1> | 81.3 |
LiAlO2 (mp-3427) | <1 0 0> | <0 0 1> | 162.6 |
LiAlO2 (mp-3427) | <1 0 1> | <1 1 0> | 171.8 |
Fe2O3 (mp-24972) | <1 0 1> | <0 1 0> | 222.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.3999 | 0.023 | 3 |
Co5(P3O11)2 (mp-31617) | 0.3757 | 0.034 | 3 |
Fe5(P3O11)2 (mp-31872) | 0.4351 | 0.038 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.3446 | 0.082 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.3996 | 0.038 | 3 |
Li5Co9(P2O7)8 (mp-705379) | 0.3272 | 0.079 | 4 |
LiVP2O7 (mp-18911) | 0.3296 | 0.033 | 4 |
LiScP2O7 (mp-10517) | 0.3388 | 0.000 | 4 |
LiTiP2O7 (mp-26629) | 0.3249 | 0.055 | 4 |
LiCoP2O7 (mp-31535) | 0.3396 | 0.057 | 4 |
LiMnV(P2O7)2 (mp-764615) | 0.0441 | 0.007 | 5 |
LiMnV(P2O7)2 (mp-764488) | 0.0659 | 0.007 | 5 |
LiMnV(P2O7)2 (mp-764480) | 0.0400 | 0.007 | 5 |
LiMnV(P2O7)2 (mp-764484) | 0.0260 | 0.006 | 5 |
LiMnV(P2O7)2 (mp-764622) | 0.0683 | 0.005 | 5 |
KLiMnP3HO10 (mp-764313) | 0.7484 | 0.046 | 6 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5377 | 0.255 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5047 | 0.330 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5781 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P O |
Final Energy/Atom-7.2621 eV |
Corrected Energy-662.7953 eV
-662.7953 eV = -610.0157 eV (uncorrected energy) - 39.3282 eV (MP Anion Correction) - 13.4514 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)