Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.847 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.035 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVO2 + LiF |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [160] |
HallR 3 2" |
Point Groupm |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 208.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 327.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 238.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 268.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 208.4 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 238.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 208.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 119.1 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 172.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 89.3 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 327.6 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 208.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 258.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 238.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 172.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 208.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 238.2 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 238.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 148.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 119.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 208.4 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 357.3 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 148.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 29.8 |
YVO4 (mp-19133) | <0 0 1> | <1 1 1> | 152.2 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 149.2 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 258.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 208.4 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.0 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 327.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 119.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 29.8 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 238.2 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 172.3 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 148.9 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 208.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 89.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 208.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 119.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 89.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 238.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 268.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 119.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 268.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 327.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 268.0 |
BN (mp-984) | <1 1 1> | <1 0 1> | 273.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe35SiO48 (mp-762943) | 0.2974 | 0.490 | 3 |
Fe7(SiO6)2 (mp-763339) | 0.3135 | 0.713 | 3 |
Mg(BiO2)2 (mvc-9468) | 0.3069 | 0.195 | 3 |
Zn(BiO2)2 (mvc-9588) | 0.3338 | 0.176 | 3 |
Mg(BiO2)2 (mvc-9719) | 0.3113 | 0.186 | 3 |
Li7V6Ni5O24 (mp-769574) | 0.3107 | 0.013 | 4 |
LiMnVO4 (mp-861571) | 0.3294 | 0.024 | 4 |
LiVSiO4 (mp-767033) | 0.3257 | 0.041 | 4 |
LiCrSiO4 (mp-763701) | 0.3183 | 0.059 | 4 |
LiVCoO4 (mp-768046) | 0.3391 | 0.000 | 4 |
Fe3O4 (mp-715491) | 0.4193 | 0.017 | 2 |
Cr3N4 (mp-1014358) | 0.4230 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.4143 | 0.060 | 2 |
Fe3O4 (mp-715558) | 0.4253 | 0.785 | 2 |
Fe3O4 (mp-716052) | 0.4191 | 0.781 | 2 |
Li4Cr3Ni3(TeO8)2 (mp-761407) | 0.4089 | 0.179 | 5 |
Li4Cr3Co3(TeO8)2 (mp-775136) | 0.3955 | 0.062 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.4093 | 0.197 | 5 |
Li4V3Ni2Sn3O16 (mp-777392) | 0.4050 | 0.081 | 5 |
Li4Nb3V3(SnO8)2 (mp-767976) | 0.3904 | 0.129 | 5 |
Li3MnFeCo(PO4)3 (mp-764931) | 0.5168 | 0.017 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.5042 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.5161 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764707) | 0.5190 | 0.035 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.5172 | 0.057 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-6.0689 eV |
Corrected Energy-182.2741 eV
-182.2741 eV = -169.9278 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)