Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.039 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2VOF4 |
Band Gap1.599 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmc21 [36] |
HallC 2c 2 |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 262.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 255.8 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 225.0 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 112.5 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 261.8 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 109.6 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 300.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 109.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 328.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 255.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 337.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 219.3 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 112.5 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 109.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 219.6 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 109.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 146.2 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 109.6 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 328.9 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 150.0 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 209.4 |
KCl (mp-23193) | <1 1 0> | <0 1 0> | 112.5 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 314.2 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 146.2 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 262.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 261.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 261.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 261.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 207.1 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 262.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 103.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 209.4 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 255.8 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 75.0 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 261.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 73.1 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 112.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 262.5 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 73.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 225.0 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 209.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 109.6 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 109.6 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 255.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 182.7 |
BN (mp-984) | <1 0 1> | <0 0 1> | 255.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 187.5 |
LiNbO3 (mp-3731) | <1 1 0> | <0 1 1> | 261.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 187.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 292.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.07480 |
-0.22302 | 0.81452 | -1.04011 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.17149 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max1.33978 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.41 | 0.00 | 0.00 |
0.00 | 2.37 | 0.00 |
0.00 | 0.00 | 5.26 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.35 | 0.00 | 0.00 |
0.00 | 24.25 | 0.00 |
0.00 | 0.00 | 12.84 |
Polycrystalline dielectric constant
εpoly∞
3.35
|
Polycrystalline dielectric constant
εpoly
14.81
|
Refractive Index n1.83 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2VF5 (mp-767661) | 0.5622 | 0.042 | 3 |
Li2CuF5 (mp-759235) | 0.5324 | 0.025 | 3 |
V3SnO8 (mp-778681) | 0.5732 | 0.070 | 3 |
V3CrO8 (mp-849352) | 0.5638 | 0.042 | 3 |
Ag2BiO3 (mp-561113) | 0.5388 | 0.001 | 3 |
Li2VOF4 (mp-780857) | 0.4990 | 0.000 | 4 |
Li11V6O5F19 (mp-779345) | 0.5317 | 0.167 | 4 |
Li3V4(OF3)3 (mp-777658) | 0.4973 | 0.103 | 4 |
Li3V4(OF3)3 (mp-779822) | 0.4787 | 0.089 | 4 |
Li3V4(OF3)3 (mp-779205) | 0.5473 | 0.091 | 4 |
TiO2 (mp-554278) | 0.6953 | 0.000 | 2 |
VO2 (mp-561637) | 0.5986 | 0.020 | 2 |
Ti6O11 (mp-559964) | 0.6912 | 0.008 | 2 |
Ti3O5 (mp-556480) | 0.7094 | 0.009 | 2 |
CeSe2 (mp-1080321) | 0.6834 | 0.140 | 2 |
Li7Zr3Nb(TeO6)4 (mp-766103) | 0.6329 | 0.012 | 5 |
Li4SbTe2WO12 (mp-765930) | 0.6939 | 0.086 | 5 |
Li3ZrNb(TeO6)2 (mp-754249) | 0.6484 | 0.021 | 5 |
Li7Zr3Nb(TeO6)4 (mp-695434) | 0.6031 | 0.018 | 5 |
LaZnCrCoO6 (mvc-9866) | 0.6723 | 0.162 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-5.6820 eV |
Corrected Energy-95.6803 eV
-95.6803 eV = -90.9117 eV (uncorrected energy) - 3.3640 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|