Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.981 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.093 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2VOF4 + LiF |
Band Gap2.991 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinImm2 [44] |
HallI 2 2 |
Point Groupm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 169.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 279.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 279.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 1> | 172.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 165.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 39.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 56.6 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 206.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 279.4 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 172.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 319.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 319.3 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 321.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 240.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 39.9 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 56.6 |
KCl (mp-23193) | <1 1 1> | <0 1 1> | 283.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 339.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 172.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 330.0 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 113.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 159.6 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 165.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 82.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 359.2 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 226.5 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 206.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 82.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 114.8 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 280.2 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 199.5 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 199.5 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 206.3 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 226.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 199.5 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 41.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 119.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 199.5 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 280.2 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 280.2 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 279.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 159.6 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 226.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 206.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 123.8 |
GaSe (mp-1943) | <1 0 1> | <0 1 1> | 283.1 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 115.1 |
BN (mp-984) | <0 0 1> | <0 1 0> | 281.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 247.5 |
BN (mp-984) | <1 1 0> | <1 1 1> | 70.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 1.53770 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | -0.05705 | 0.00000 | 0.00000 |
-0.06257 | -0.12979 | -0.43885 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max1.53770 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.10 | 0.00 | 0.00 |
0.00 | 2.13 | 0.00 |
0.00 | 0.00 | 2.41 |
Dielectric Tensor εij (total) |
||
---|---|---|
19.18 | 0.00 | 0.00 |
0.00 | 3.87 | 0.00 |
0.00 | 0.00 | 4.38 |
Polycrystalline dielectric constant
εpoly∞
2.21
|
Polycrystalline dielectric constant
εpoly
9.14
|
Refractive Index n1.49 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ag2Mo2O7 (mp-504777) | 0.7442 | 0.000 | 3 |
Sn3WO6 (mp-566092) | 0.5470 | 0.047 | 3 |
Nb2CrO8 (mvc-480) | 0.7369 | 0.256 | 3 |
Co5Te4(ClO6)2 (mp-687152) | 0.7006 | 0.388 | 4 |
Li3V(TeO3)4 (mp-771850) | 0.6900 | 0.071 | 4 |
Ni5Te4(ClO6)2 (mp-565798) | 0.7032 | 0.000 | 4 |
Ca2Nb2SnO8 (mvc-81) | 0.6742 | 0.091 | 4 |
Ca2Ta2SnO8 (mvc-2394) | 0.6471 | 0.100 | 4 |
Bi2O3 (mp-674644) | 0.7109 | 0.638 | 2 |
SrCo2Te3(ClO4)2 (mp-646431) | 0.7302 | 0.087 | 5 |
CaCo2Te3(ClO4)2 (mp-646538) | 0.7137 | 0.068 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-5.4287 eV |
Corrected Energy-113.3426 eV
-113.3426 eV = -108.5740 eV (uncorrected energy) - 3.3640 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)