Final Magnetic Moment0.235 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.380 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.037 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe3BO5 + LiFeBO3 + Li3B7O12 + Fe2O3 |
Band Gap1.683 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 160.9 |
CeO2 (mp-20194) | <1 1 1> | <0 1 1> | 213.1 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 268.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 237.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 284.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 189.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 331.9 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 142.1 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 268.2 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 331.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 331.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 237.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 142.3 |
AlN (mp-661) | <1 1 1> | <0 1 1> | 142.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 142.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 268.2 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 268.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 331.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 331.9 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 268.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 331.9 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 142.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 284.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 214.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 47.4 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 237.1 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 268.2 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 276.9 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 115.7 |
SiC (mp-7631) | <1 1 0> | <0 1 0> | 160.9 |
SiC (mp-7631) | <1 1 1> | <0 1 0> | 160.9 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 47.4 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 94.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 206.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 237.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 189.7 |
C (mp-66) | <1 1 1> | <0 1 0> | 268.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 268.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 284.5 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 268.2 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 212.9 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 268.2 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 331.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 268.2 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 106.5 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 106.5 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 276.9 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 237.1 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 284.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 94.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li6B4O9 (mp-768875) | 0.6118 | 0.063 | 3 |
Na3CoO3 (mp-777919) | 0.6102 | 0.127 | 3 |
Li6B4O9 (mp-1020024) | 0.6210 | 0.000 | 3 |
Li3Fe4(BO3)4 (mp-764932) | 0.1438 | 0.028 | 4 |
Li3Fe4(BO3)4 (mp-764888) | 0.1440 | 0.024 | 4 |
Li5Fe8(BO3)8 (mp-764614) | 0.1356 | 0.036 | 4 |
Li3Fe4(BO3)4 (mp-764586) | 0.0684 | 0.038 | 4 |
Li3Fe4(BO3)4 (mp-764502) | 0.1300 | 0.018 | 4 |
Li8MnFe7(BO3)8 (mp-850743) | 0.3923 | 0.017 | 5 |
Li4MnFe2(BO3)4 (mp-767642) | 0.3681 | 0.055 | 5 |
Li8MnFe7(BO3)8 (mp-780443) | 0.4056 | 0.000 | 5 |
Li8Mn3Fe5(BO3)8 (mp-775252) | 0.3924 | 0.012 | 5 |
Li2MnFe(BO3)2 (mp-779099) | 0.4060 | 0.011 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv B O |
Final Energy/Atom-6.9878 eV |
Corrected Energy-355.9752 eV
Uncorrected energy = -321.4392 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-2.256 eV/atom x 8.0 atoms) = -18.0480 eV
Corrected energy = -355.9752 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)