Final Magnetic Moment17.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.594 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToFe2O3 + FeF2 + FeF3 |
Band Gap1.852 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 279.2 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 311.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 139.6 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 1> | 124.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 279.2 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 278.9 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 55.8 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 307.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 167.5 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 244.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 251.2 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 205.1 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 187.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 244.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 195.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 167.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 260.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 208.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 139.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 260.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 335.0 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 311.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 139.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 249.5 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 195.4 |
YVO4 (mp-19133) | <1 0 0> | <1 0 1> | 187.1 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 208.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 195.4 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 139.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 249.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 251.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 195.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 195.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 362.9 |
Te2W (mp-22693) | <1 0 1> | <0 0 1> | 195.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 162.7 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 167.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 362.9 |
BN (mp-984) | <1 0 0> | <0 0 1> | 195.4 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 195.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 139.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 307.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 279.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 195.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 251.2 |
Al (mp-134) | <1 1 1> | <1 0 1> | 249.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 195.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 -1> | 334.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe3OF5 (mp-779917) | 0.1217 | 0.064 | 3 |
Fe4OF7 (mp-779881) | 0.1146 | 0.059 | 3 |
Fe4OF7 (mp-778724) | 0.1147 | 0.070 | 3 |
Fe4OF7 (mp-778570) | 0.1233 | 0.058 | 3 |
Fe4OF7 (mp-763484) | 0.1039 | 0.057 | 3 |
LiFe2OF5 (mp-779997) | 0.1860 | 0.026 | 4 |
LiFe2OF5 (mp-779300) | 0.1859 | 0.054 | 4 |
LiMn3(OF3)2 (mp-767084) | 0.1747 | 0.018 | 4 |
AlCr(WO4)2 (mvc-684) | 0.1995 | 0.046 | 4 |
AlFe(WO4)2 (mvc-836) | 0.2053 | 0.069 | 4 |
TiO2 (mp-775938) | 0.2588 | 0.039 | 2 |
ZrO2 (mp-775980) | 0.2765 | 0.051 | 2 |
SiO2 (mp-32667) | 0.2608 | 0.241 | 2 |
HfO2 (mp-776097) | 0.2766 | 0.028 | 2 |
VO2 (mp-25145) | 0.2797 | 0.055 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv O F |
Final Energy/Atom-5.6889 eV |
Corrected Energy-159.8022 eV
-159.8022 eV = -136.5336 eV (uncorrected energy) - 21.8640 eV (MP Advanced Correction) - 1.4046 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)