Final Magnetic Moment15.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.072 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.066 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.81 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr2CoO4 + LiCoSbO4 + Li3SbO4 + LiSbO3 |
Band Gap0.645 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 302.1 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 323.0 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 266.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 193.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 181.2 |
GaN (mp-804) | <1 0 1> | <1 0 1> | 266.2 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 258.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 323.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 207.8 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 193.8 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 266.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 241.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 207.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 323.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 258.4 |
YVO4 (mp-19133) | <1 0 1> | <0 1 0> | 207.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 323.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 323.0 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 193.8 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 193.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 258.4 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 302.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 302.1 |
BN (mp-984) | <1 1 1> | <1 0 0> | 302.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 193.8 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 266.2 |
Al (mp-134) | <1 1 0> | <0 1 0> | 207.8 |
MoS2 (mp-1434) | <1 0 0> | <0 1 0> | 207.8 |
Al (mp-134) | <1 0 0> | <1 0 0> | 241.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 323.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 129.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 64.6 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 266.2 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 181.2 |
SiC (mp-7631) | <1 0 1> | <0 0 1> | 193.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 193.8 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 129.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 302.1 |
C (mp-66) | <1 1 0> | <1 0 0> | 181.2 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 181.2 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 302.1 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 258.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 181.2 |
LaF3 (mp-905) | <0 0 1> | <0 0 1> | 129.2 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 323.0 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 181.2 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 258.4 |
InP (mp-20351) | <1 0 0> | <1 0 1> | 177.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 258.4 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 258.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe2CuO4 (mp-705659) | 0.3162 | 0.589 | 3 |
Ca(MoO2)2 (mvc-10002) | 0.3229 | 0.276 | 3 |
MgMn2O4 (mvc-10190) | 0.3236 | 0.549 | 3 |
Ca(WO2)2 (mvc-10243) | 0.2673 | 0.458 | 3 |
Ca(WO2)2 (mvc-10486) | 0.2237 | 0.499 | 3 |
Li4Mn5Nb3O16 (mp-773388) | 0.2230 | 0.724 | 4 |
Li4Co3Sb5O16 (mp-770677) | 0.2394 | 0.057 | 4 |
Li4Mn5Sb3O16 (mp-769848) | 0.1915 | 0.112 | 4 |
Li4Mn5V3O16 (mp-773194) | 0.2230 | 0.230 | 4 |
Li4Co5Sb3O16 (mp-771118) | 0.2376 | 0.225 | 4 |
Si3N4 (mp-641539) | 0.5194 | 0.288 | 2 |
Ge3N4 (mp-641541) | 0.4817 | 0.208 | 2 |
Fe3O4 (mp-542433) | 0.5280 | 0.075 | 2 |
Fe3O4 (mp-650112) | 0.5089 | 0.060 | 2 |
Fe3O4 (mp-716052) | 0.5269 | 0.781 | 2 |
Li4Nb3Fe3(NiO8)2 (mp-775068) | 0.1249 | 0.118 | 5 |
Li4V3Co2Sb3O16 (mp-770636) | 0.0870 | 0.122 | 5 |
Li4Cr3Fe2Sb3O16 (mp-773763) | 0.1025 | 0.592 | 5 |
Li4V3Fe2Sb3O16 (mp-853181) | 0.1177 | 0.341 | 5 |
Li4Cr3Ni2Sb3O16 (mp-769736) | 0.1299 | 0.071 | 5 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.7497 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Co Sb O |
Final Energy/Atom-6.4054 eV |
Corrected Energy-200.3741 eV
-200.3741 eV = -179.3505 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 9.7870 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)