Final Magnetic Moment2.500 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.699 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.061 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO + MnF2 + LiF |
Band Gap1.856 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group2/m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 287.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 34.5 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 143.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 199.1 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 241.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 239.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 331.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 241.7 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 199.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 165.9 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 143.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 241.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 232.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 310.7 |
InAs (mp-20305) | <1 0 0> | <1 0 1> | 191.6 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 335.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 241.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 232.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 103.6 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 99.6 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 287.4 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 239.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 66.4 |
Te2W (mp-22693) | <1 0 0> | <1 0 1> | 95.8 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 99.6 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 265.5 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 66.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 310.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 172.5 |
TePb (mp-19717) | <1 1 1> | <1 0 0> | 298.7 |
Te2Mo (mp-602) | <1 1 0> | <1 0 1> | 95.8 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 33.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 138.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 57.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 335.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 241.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 1> | 335.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 287.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 165.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 172.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 310.7 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 165.9 |
BN (mp-984) | <0 0 1> | <0 0 1> | 103.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 99.6 |
BN (mp-984) | <1 1 0> | <1 0 1> | 335.2 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 239.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 241.7 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 232.3 |
Al (mp-134) | <1 1 0> | <1 0 0> | 232.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 232.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5CuF8 (mp-753202) | 0.3349 | 0.002 | 3 |
Fe2SiS4 (mp-1024054) | 0.3394 | 0.209 | 3 |
Ca(AgO2)2 (mvc-6537) | 0.3445 | 0.258 | 3 |
Mg(BiO2)2 (mvc-6512) | 0.3437 | 0.126 | 3 |
Li2Mn3WO8 (mp-772369) | 0.2836 | 0.049 | 4 |
LiMn2OF3 (mp-861572) | 0.2621 | 0.088 | 4 |
LiCo2OF3 (mp-764154) | 0.1662 | 0.083 | 4 |
LiNi2OF3 (mp-765808) | 0.2116 | 0.092 | 4 |
LiCo2OF3 (mp-765692) | 0.2844 | 0.299 | 4 |
Fe3O4 (mp-715491) | 0.4455 | 0.017 | 2 |
Si3N4 (mp-641539) | 0.4412 | 0.288 | 2 |
Mn3N4 (mp-1080204) | 0.4535 | 0.172 | 2 |
Cr3N4 (mp-1014358) | 0.3808 | 0.227 | 2 |
Fe3O4 (mp-650112) | 0.4484 | 0.060 | 2 |
Li4Mn3Ni3(TeO8)2 (mp-770951) | 0.3577 | 0.002 | 5 |
Li4Mn3Fe3(SbO8)2 (mp-775013) | 0.3447 | 0.005 | 5 |
Li4Fe3Ni3(TeO8)2 (mp-773382) | 0.3426 | 0.197 | 5 |
Li4V3Co3(WO8)2 (mp-763152) | 0.3573 | 0.263 | 5 |
Li4Fe3Co3(TeO8)2 (mp-849468) | 0.3273 | 0.067 | 5 |
Li3MnFeCo(PO4)3 (mp-764804) | 0.6512 | 0.043 | 6 |
Li3MnFeCo(PO4)3 (mp-764809) | 0.6436 | 0.014 | 6 |
Li3MnFeCo(PO4)3 (mp-764869) | 0.6508 | 0.032 | 6 |
Li3MnFeCo(PO4)3 (mp-764969) | 0.6540 | 0.057 | 6 |
Li3MnFeCo(PO4)3 (mp-764870) | 0.6507 | 0.466 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O F |
Final Energy/Atom-6.3247 eV |
Corrected Energy-193.3470 eV
-193.3470 eV = -177.0911 eV (uncorrected energy) - 13.4468 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)