Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.271 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.007 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.424 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2221 [20] |
HallC 2c 2 |
Point Group222 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <0 0 1> | <0 1 0> | 296.9 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 228.5 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 127.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 296.9 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 251.7 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 254.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 325.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 325.5 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 174.4 |
Te2W (mp-22693) | <1 0 0> | <0 1 1> | 188.8 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 46.5 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 127.2 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 84.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 339.3 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 254.5 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 261.5 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 251.7 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 178.5 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 228.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 314.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 228.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 139.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 232.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 279.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 325.5 |
Te2Mo (mp-602) | <1 1 0> | <0 1 1> | 188.8 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 212.1 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 296.9 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 339.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 212.1 |
GaN (mp-804) | <1 0 1> | <0 1 1> | 188.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 84.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 314.7 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 84.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 139.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 339.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 314.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 139.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 325.5 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 178.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 139.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 267.7 |
BN (mp-984) | <0 0 1> | <0 1 0> | 212.1 |
BN (mp-984) | <1 0 0> | <0 1 1> | 188.8 |
BN (mp-984) | <1 0 1> | <0 1 0> | 254.5 |
InAs (mp-20305) | <1 0 0> | <0 1 1> | 314.7 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 279.0 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 339.3 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 228.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 46.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | -1.41710 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.74936 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.00707 |
Piezoelectric Modulus ‖eij‖max1.41710 C/m2 |
Crystallographic Direction vmax |
---|
1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.25 | 0.00 | 0.00 |
0.00 | 2.25 | 0.00 |
0.00 | 0.00 | 2.15 |
Dielectric Tensor εij (total) |
||
---|---|---|
28.89 | 0.00 | 0.00 |
0.00 | 5.50 | 0.00 |
0.00 | 0.00 | 3.85 |
Polycrystalline dielectric constant
εpoly∞
2.22
|
Polycrystalline dielectric constant
εpoly
12.74
|
Refractive Index n1.49 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-5724) | 0.3974 | 0.003 | 3 |
AlPO4 (mp-5859) | 0.3433 | 0.011 | 3 |
AlPO4 (mp-37990) | 0.3328 | 0.014 | 3 |
AlPO4 (mp-557842) | 0.3378 | 0.011 | 3 |
AlPO4 (mp-675254) | 0.3535 | 0.012 | 3 |
CsAlSiO4 (mp-561457) | 0.6685 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.5501 | 0.000 | 4 |
CrN2 (mp-1014565) | 0.1487 | 0.345 | 2 |
SiO2 (mp-554543) | 0.1403 | 0.013 | 2 |
SiO2 (mp-600004) | 0.1491 | 0.012 | 2 |
SiO2 (mp-600018) | 0.1458 | 0.012 | 2 |
SiO2 (mp-560826) | 0.1345 | 0.012 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9088 eV |
Corrected Energy-100.5240 eV
-100.5240 eV = -94.9057 eV (uncorrected energy) - 5.6183 eV (MP Anion Correction)
|