Final Magnetic Moment2.997 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.797 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.068 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.37 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoO2 + Cr2CoO4 + Li(CoO2)2 + Li2CrO4 |
Band Gap0.225 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TePb (mp-19717) | <1 0 0> | <1 0 0> | 166.4 |
TePb (mp-19717) | <1 1 0> | <1 1 1> | 186.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 339.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 339.8 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 142.6 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 174.1 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 142.6 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 33.3 |
Ag (mp-124) | <1 1 0> | <1 0 -1> | 47.0 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 232.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 285.3 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 299.5 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 142.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 113.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 266.2 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 33.3 |
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 47.0 |
GaAs (mp-2534) | <1 1 1> | <1 0 -1> | 235.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 166.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 266.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 99.8 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 188.0 |
BN (mp-984) | <1 1 0> | <1 1 0> | 232.1 |
BN (mp-984) | <1 1 1> | <1 1 0> | 232.1 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 232.9 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 240.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 199.7 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 235.0 |
GaN (mp-804) | <1 1 1> | <0 1 1> | 147.9 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 0> | 142.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 169.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 221.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 141.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 290.2 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 166.4 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 -1> | 94.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 133.1 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 221.8 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 -1> | 47.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 56.6 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 66.6 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 1> | 73.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 113.3 |
Al (mp-134) | <1 0 0> | <1 0 0> | 33.3 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 47.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 56.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 299.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 33.3 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 47.0 |
ZnSe (mp-1190) | <1 1 1> | <1 0 -1> | 235.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li3(CoO2)4 (mp-763750) | 0.2189 | 0.140 | 3 |
Li3Cr4O8 (mp-771288) | 0.1893 | 0.034 | 3 |
Li3(CoO2)4 (mp-853206) | 0.1475 | 0.109 | 3 |
Li3(NiO2)4 (mvc-16810) | 0.2119 | 0.017 | 3 |
Li3(CoO2)4 (mvc-16807) | 0.1586 | 0.178 | 3 |
Li3VCr3O8 (mp-780821) | 0.1412 | 0.118 | 4 |
Li3Mn2(CoO4)2 (mp-779153) | 0.1254 | 0.105 | 4 |
Li3Mn3CoO8 (mp-765796) | 0.1492 | 0.077 | 4 |
Li3MnCo3O8 (mp-762866) | 0.1108 | 0.105 | 4 |
Li3Ti3VO8 (mp-762821) | 0.1492 | 0.059 | 4 |
Fe8O9 (mp-763787) | 0.2622 | 0.063 | 2 |
Fe9O10 (mp-763441) | 0.2816 | 0.350 | 2 |
Fe7O8 (mp-715333) | 0.2567 | 0.064 | 2 |
Fe8O9 (mp-705588) | 0.2847 | 0.050 | 2 |
Fe10O11 (mp-705555) | 0.2987 | 0.046 | 2 |
Li6Mn3Cr2Fe3O16 (mp-861553) | 0.4286 | 0.882 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eVCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Cr_pv Co O |
Final Energy/Atom-5.9995 eV |
Corrected Energy-206.4920 eV
-206.4920 eV = -179.9854 eV (uncorrected energy) - 15.2700 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)