Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.271 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.069 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.31 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi5FeO4 + Li2O + LiF + Fe |
Band Gap2.902 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 223.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 223.7 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 124.2 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 162.8 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 195.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 -1> | 146.5 |
GaAs (mp-2534) | <1 0 0> | <1 -1 -1> | 234.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 186.2 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 244.1 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 279.5 |
AlN (mp-661) | <1 0 0> | <1 -1 1> | 45.7 |
AlN (mp-661) | <1 1 0> | <0 1 -1> | 183.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 260.5 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 260.5 |
GaAs (mp-2534) | <1 1 1> | <1 -1 1> | 274.4 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 341.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 217.4 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 186.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 212.8 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 227.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 239.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 292.6 |
SiO2 (mp-6930) | <1 0 0> | <1 -1 0> | 165.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 279.5 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 93.2 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 244.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 -1 -1> | 117.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 159.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 203.7 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 195.2 |
CdS (mp-672) | <1 0 0> | <1 -1 -1> | 195.0 |
CdS (mp-672) | <1 0 1> | <0 1 1> | 134.2 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 162.8 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 67.8 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 203.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 195.2 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 268.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 156.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 0> | 132.6 |
DyScO3 (mp-31120) | <0 1 1> | <1 -1 0> | 165.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 -1 -1> | 234.0 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 0> | 165.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 -1> | 260.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 292.6 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 239.4 |
YVO4 (mp-19133) | <1 0 1> | <1 -1 -1> | 273.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 293.1 |
InAs (mp-20305) | <1 1 0> | <1 0 -1> | 271.7 |
ZnSe (mp-1190) | <1 0 0> | <1 -1 -1> | 234.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 186.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaNa2O2 (mp-756521) | 0.6228 | 0.089 | 3 |
Li5SbS4 (mp-775817) | 0.6503 | 0.060 | 3 |
Li5MnO4 (mp-770514) | 0.6700 | 0.085 | 3 |
Li2MnF4 (mp-777864) | 0.6698 | 0.055 | 3 |
Li8Ti2O7 (mp-772920) | 0.6699 | 0.070 | 3 |
Ca2YSnO5 (mvc-6291) | 0.6762 | 0.182 | 4 |
Li7Mn(O2F)2 (mp-767574) | 0.6689 | 0.285 | 4 |
Li3CoO2F (mp-763914) | 0.7104 | 0.070 | 4 |
Li3NiO2F (mp-765537) | 0.6114 | 0.097 | 4 |
Li3FeO2F (mp-764597) | 0.6430 | 0.063 | 4 |
Sr4N3 (mp-685023) | 0.7380 | 0.191 | 2 |
V2O3 (mp-777698) | 0.7354 | 0.083 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-4.9934 eV |
Corrected Energy-321.7744 eV
-321.7744 eV = -299.6057 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)