Final Magnetic Moment3.377 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.544 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.168 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.14 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiVPO5 + Li6V3P8O29 + Li11V8(PO4)12 + LiMnPO4 + Li3PO4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 222.9 |
CeO2 (mp-20194) | <1 1 1> | <1 -1 -1> | 254.2 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 242.2 |
GaSe (mp-1943) | <0 0 1> | <1 -1 -1> | 254.2 |
BN (mp-984) | <0 0 1> | <0 1 0> | 212.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 263.5 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 0> | 307.4 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 263.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 242.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 1> | 242.2 |
CdTe (mp-406) | <1 1 0> | <1 -1 -1> | 254.2 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 212.5 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 297.2 |
SiC (mp-7631) | <0 0 1> | <0 1 -1> | 205.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 263.5 |
MgO (mp-1265) | <1 0 0> | <0 1 1> | 161.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 263.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 222.9 |
TiO2 (mp-2657) | <1 1 0> | <1 -1 -1> | 254.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 316.1 |
C (mp-66) | <1 1 0> | <0 1 -1> | 273.6 |
C (mp-66) | <1 1 1> | <0 0 1> | 263.5 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 316.1 |
GdScO3 (mp-5690) | <1 0 1> | <1 0 0> | 222.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 161.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 80.7 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 222.9 |
BaF2 (mp-1029) | <1 1 1> | <0 1 0> | 265.6 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 153.3 |
GaN (mp-804) | <1 0 1> | <1 -1 -1> | 169.4 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 207.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 263.5 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 80.7 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 222.9 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 316.1 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 222.9 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 222.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 263.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 161.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 318.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 210.8 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 230.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 263.5 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 260.0 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 222.9 |
Te2W (mp-22693) | <1 0 0> | <1 0 0> | 297.2 |
YVO4 (mp-19133) | <1 1 0> | <1 1 1> | 130.0 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 210.8 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 260.0 |
BN (mp-984) | <1 0 0> | <1 0 0> | 297.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2PO5 (mp-771449) | 0.5224 | 1.293 | 3 |
CdGeO3 (mp-2951) | 0.5767 | 0.001 | 3 |
Li2Cr2O7 (mp-770745) | 0.5867 | 0.068 | 3 |
VSiO3 (mp-769952) | 0.5636 | 0.019 | 3 |
Na2W2O7 (mp-25800) | 0.5872 | 0.021 | 3 |
LiCu4(PO4)3 (mp-761193) | 0.3753 | 0.084 | 4 |
Li3Ti2(PO4)3 (mp-758287) | 0.3401 | 0.098 | 4 |
Li3Ni2(PO4)3 (mp-504123) | 0.3761 | 0.072 | 4 |
Na3Fe2(MoO4)3 (mp-560526) | 0.3599 | 0.220 | 4 |
Li3V2(PO4)3 (mp-540455) | 0.4196 | 0.085 | 4 |
Li6MnV3(PO4)6 (mp-764970) | 0.0923 | 0.204 | 5 |
Li6MnV3(PO4)6 (mp-764485) | 0.1097 | 0.114 | 5 |
Li3MnV(PO4)3 (mp-779830) | 0.1155 | 0.246 | 5 |
Li6MnV3(PO4)6 (mp-764756) | 0.0751 | 0.154 | 5 |
Li6MnV3(PO4)6 (mp-779207) | 0.1113 | 0.177 | 5 |
Li4CrCo2Ni3(PO4)6 (mp-776777) | 0.6338 | 0.086 | 6 |
Li4Mn3CrCo2(PO4)6 (mp-763479) | 0.6414 | 0.080 | 6 |
Li2Mg2MnFe(PO4)4 (mp-849669) | 0.5530 | 0.008 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6244 | 0.018 | 6 |
Li4CrFe2Ni3(PO4)6 (mp-776753) | 0.6168 | 0.778 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P O |
Final Energy/Atom-6.9323 eV |
Corrected Energy-300.8729 eV
-300.8729 eV = -277.2911 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 6.7269 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)