Final Magnetic Moment0.254 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.521 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.159 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.88 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6V3P8O29 + Mn2P2O7 + Mn(PO3)2 |
Band Gap0.396 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 326.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 260.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 163.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 195.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 260.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 326.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 358.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 228.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 293.6 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 326.2 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 358.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 293.6 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 293.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 260.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 293.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 130.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 326.2 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 293.6 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 326.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 228.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 195.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 260.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 228.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 175.7 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 228.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 260.9 |
YVO4 (mp-19133) | <1 1 1> | <0 1 1> | 250.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 293.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 175.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 293.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 97.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 358.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 260.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 228.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 326.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 228.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 260.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 260.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 195.7 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 260.9 |
Al (mp-134) | <1 1 0> | <0 0 1> | 228.3 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 293.6 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 260.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 326.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 228.3 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 260.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 358.8 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 326.2 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 358.8 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 293.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V5(P3O11)2 (mp-767351) | 0.4271 | 0.020 | 3 |
Co5(P3O11)2 (mp-31617) | 0.4557 | 0.031 | 3 |
Ni5(P3O11)2 (mp-32359) | 0.3566 | 0.098 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.4468 | 0.065 | 3 |
Fe5(P3O11)2 (mp-705342) | 0.4312 | 0.366 | 3 |
LiVP2O7 (mp-18911) | 0.1203 | 0.025 | 4 |
LiMoP2O7 (mp-18987) | 0.1894 | 0.052 | 4 |
LiCrP2O7 (mp-19103) | 0.1606 | 0.070 | 4 |
LiFeP2O7 (mp-19294) | 0.1386 | 0.164 | 4 |
LiScP2O7 (mp-10517) | 0.1382 | 0.000 | 4 |
Li4MnV3(P2O7)4 (mp-850462) | 0.0425 | 0.087 | 5 |
Li4MnV3(P2O7)4 (mp-778342) | 0.0441 | 0.007 | 5 |
Li2MnV(P2O7)2 (mp-779842) | 0.0319 | 0.024 | 5 |
Li2MnV(P2O7)2 (mp-774309) | 0.0426 | 0.084 | 5 |
Li4MnV3(P2O7)4 (mp-780005) | 0.0369 | 0.000 | 5 |
LiMgCr3Se2(SO6)4 (mp-769552) | 0.5853 | 0.003 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.5119 | 0.041 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.5540 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P O |
Final Energy/Atom-7.0574 eV |
Corrected Energy-505.3732 eV
-505.3732 eV = -465.7885 eV (uncorrected energy) - 29.4962 eV (MP Anion Correction) - 10.0886 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)