Final Magnetic Moment
2.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-3.213 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.024 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.85 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
LiVF4
Band Gap
2.328 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P21 [4]
Hall
P 2yb
Point Group
2
Crystal System
monoclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <0 0 1> 0.004 87.9
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.006 129.1
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.006 87.9
WS2 (mp-224) <0 0 1> <0 0 1> 0.007 87.9
NaCl (mp-22862) <1 1 1> <1 0 -1> 0.007 224.7
TiO2 (mp-2657) <1 1 0> <1 0 0> 0.010 156.9
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.011 87.9
AlN (mp-661) <1 0 1> <1 0 0> 0.011 125.5
WS2 (mp-224) <1 1 0> <0 0 1> 0.012 234.3
MoS2 (mp-1434) <1 1 0> <0 0 1> 0.015 117.2
MgF2 (mp-1249) <1 1 1> <1 1 0> 0.022 301.1
GaN (mp-804) <1 1 0> <0 0 1> 0.025 29.3
ZnO (mp-2133) <0 0 1> <1 1 -1> 0.031 130.7
GdScO3 (mp-5690) <0 1 0> <0 0 1> 0.035 87.9
TbScO3 (mp-31119) <0 1 0> <0 0 1> 0.039 87.9
YAlO3 (mp-3792) <0 1 0> <0 0 1> 0.043 117.2
TeO2 (mp-2125) <0 1 0> <0 0 1> 0.044 205.0
Ga2O3 (mp-886) <1 1 0> <0 1 0> 0.044 147.2
Mg (mp-153) <1 1 0> <0 0 1> 0.047 29.3
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.051 86.0
Ag (mp-124) <1 1 1> <1 1 0> 0.051 301.1
CdS (mp-672) <0 0 1> <1 1 0> 0.051 215.1
CsI (mp-614603) <1 1 1> <1 1 0> 0.051 215.1
SrTiO3 (mp-4651) <1 0 1> <1 1 0> 0.052 215.1
Au (mp-81) <1 1 1> <1 1 0> 0.056 301.1
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.059 219.6
LiTaO3 (mp-3666) <1 0 0> <0 0 1> 0.062 146.5
Bi2Se3 (mp-541837) <0 0 1> <1 1 0> 0.062 215.1
CeO2 (mp-20194) <1 1 1> <1 1 0> 0.063 258.1
Si (mp-149) <1 1 1> <1 1 0> 0.065 258.1
NdGaO3 (mp-3196) <1 1 1> <1 0 1> 0.065 206.1
SiC (mp-11714) <1 1 1> <1 0 0> 0.067 219.6
LiNbO3 (mp-3731) <1 0 1> <1 0 1> 0.067 154.6
MoS2 (mp-1434) <1 0 0> <1 0 1> 0.067 206.1
YAlO3 (mp-3792) <0 1 1> <1 0 -1> 0.068 96.3
C (mp-48) <0 0 1> <0 1 0> 0.069 147.2
DyScO3 (mp-31120) <0 1 0> <0 0 1> 0.071 87.9
Cu (mp-30) <1 1 1> <1 1 0> 0.076 344.2
LiTaO3 (mp-3666) <1 0 1> <1 0 1> 0.077 154.6
C (mp-48) <1 0 0> <1 0 1> 0.077 154.6
Al (mp-134) <1 1 0> <1 0 -1> 0.078 160.5
SiC (mp-7631) <1 0 1> <1 1 1> 0.081 237.3
Ni (mp-23) <1 1 0> <0 1 0> 0.086 88.3
ZrO2 (mp-2858) <1 0 -1> <0 0 1> 0.087 146.5
ZnSe (mp-1190) <1 1 1> <1 0 -1> 0.087 224.7
ZnO (mp-2133) <1 0 0> <1 0 1> 0.087 51.5
NdGaO3 (mp-3196) <1 0 0> <0 0 1> 0.087 87.9
PbS (mp-21276) <1 0 0> <1 1 0> 0.088 215.1
Fe3O4 (mp-19306) <1 1 1> <1 0 -1> 0.090 128.4
CdWO4 (mp-19387) <1 1 1> <0 1 1> 0.092 207.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.

Once you have registered you can also "vote" for full calculation of this material's elastic properties.

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
LiMnF4 (mp-778553) 0.6393 0.059 3
V(SbO3)4 (mp-770857) 0.6553 0.046 3
LiVF4 (mp-766861) 0.6218 0.062 3
LiCrF4 (mp-763488) 0.5652 0.033 3
Li3V2F9 (mp-776092) 0.5792 0.078 3
LiV2OF5 (mp-777617) 0.5902 0.072 4
Li4V3OF11 (mp-780283) 0.5970 0.042 4
LiV2OF5 (mp-777084) 0.6370 0.070 4
LiV2OF5 (mp-778861) 0.6391 0.067 4
LiNi(WO4)2 (mp-25603) 0.6262 0.090 4
Ba3LiTi5Nb3O21 (mp-686745) 0.7275 0.015 5
Ba3LiTi5(SbO7)3 (mp-695259) 0.7459 0.034 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
V: 3.25 eV
Pseudopotentials
VASP PAW: Li_sv V_pv F
Final Energy/Atom
-5.7118 eV
Corrected Energy
-71.9057 eV
-71.9057 eV = -68.5417 eV (uncorrected energy) - 3.3640 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations