Final Magnetic Moment28.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.862 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.079 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.29 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi5FeO4 + Li2MnO3 + LiFeO2 + NiO + Ni |
Band Gap0.542 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaN (mp-804) | <1 0 1> | <1 0 1> | 171.2 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 118.0 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 233.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 123.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 246.3 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 100.7 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 201.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 307.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 292.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 246.3 |
LiF (mp-1138) | <1 1 1> | <1 1 0> | 116.5 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 201.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 175.7 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 264.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 234.3 |
BN (mp-984) | <1 1 0> | <0 1 1> | 236.1 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 123.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 61.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 184.7 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 307.9 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 1> | 256.8 |
Al (mp-134) | <1 0 0> | <0 0 1> | 246.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 307.9 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 236.1 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 307.9 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 123.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 184.7 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 175.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 61.6 |
C (mp-66) | <1 0 0> | <1 0 1> | 256.8 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 100.7 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 171.2 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 264.3 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 175.7 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 246.3 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 175.7 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 292.8 |
BaTiO3 (mp-5986) | <1 0 1> | <1 0 0> | 117.1 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 184.7 |
Ga2O3 (mp-886) | <1 1 0> | <1 0 0> | 292.8 |
Au (mp-81) | <1 0 0> | <1 0 0> | 175.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 61.6 |
C (mp-48) | <0 0 1> | <0 0 1> | 307.9 |
WSe2 (mp-1821) | <1 0 1> | <1 0 0> | 292.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 234.3 |
SiC (mp-7631) | <1 0 0> | <1 1 0> | 233.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 184.7 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 1> | 256.8 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 236.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 307.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5(NiO2)4 (mp-780518) | 0.3808 | 0.327 | 3 |
Li5(FeO2)4 (mp-780312) | 0.2216 | 0.259 | 3 |
Li5(CoO2)4 (mp-780140) | 0.3055 | 0.251 | 3 |
Li5Cr4O8 (mp-850237) | 0.3449 | 0.101 | 3 |
Li5Mn4O8 (mp-849676) | 0.5856 | 0.966 | 3 |
Li10Mn3Cr5O16 (mp-765030) | 0.1962 | 0.084 | 4 |
Li10Mn3V5O16 (mp-764265) | 0.2031 | 0.587 | 4 |
Li10V3Cr5O16 (mp-764096) | 0.1772 | 0.100 | 4 |
Li10Fe5Co3O16 (mp-763869) | 0.1952 | 0.090 | 4 |
Li5V3CrO8 (mp-764013) | 0.2343 | 0.481 | 4 |
Ti3N4 (mp-1080192) | 0.7304 | 0.101 | 2 |
Li10Fe2Co3Ni3O16 (mp-780632) | 0.2013 | 0.142 | 5 |
Li10Fe3Co2Ni3O16 (mp-779868) | 0.1882 | 0.302 | 5 |
Li10Cr3Co2Ni3O16 (mp-778771) | 0.2068 | 0.263 | 5 |
Li10Mn2Fe3Co3O16 (mp-777706) | 0.2294 | 0.092 | 5 |
Li10Cr2Fe3Co3O16 (mp-774310) | 0.1608 | 0.811 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVFe: 5.3 eV Ni: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Fe_pv Ni_pv O |
Final Energy/Atom-5.6863 eV |
Corrected Energy-222.6228 eV
-222.6228 eV = -193.3335 eV (uncorrected energy) - 18.0527 eV (MP Advanced Correction) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)