Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.818 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVF5 |
Band Gap2.817 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 278.1 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 203.7 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 246.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 92.1 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 130.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 65.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 46.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 230.3 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 185.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 230.3 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 271.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 138.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 196.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 65.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 46.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 164.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 46.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 276.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 322.5 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 65.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 46.1 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 230.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 1> | 65.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 46.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 324.4 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 246.2 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 230.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 230.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 271.6 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 65.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 46.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 230.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 271.6 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 246.7 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 184.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 276.4 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 67.9 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 196.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 261.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 139.0 |
BN (mp-984) | <1 0 1> | <0 0 1> | 138.2 |
BN (mp-984) | <1 1 1> | <1 0 1> | 246.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 246.7 |
Bi2Se3 (mp-541837) | <1 0 0> | <1 0 1> | 246.2 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 139.0 |
Al (mp-134) | <1 0 0> | <0 1 1> | 65.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 46.1 |
Al (mp-134) | <1 1 1> | <0 1 0> | 324.4 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 139.0 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 184.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RuOF4 (mp-683982) | 0.4800 | 0.005 | 3 |
OsOF4 (mp-561449) | 0.4847 | 0.011 | 3 |
Ta2Hg2F11 (mp-581413) | 0.3791 | 0.000 | 3 |
OsOF4 (mp-558879) | 0.4493 | 0.013 | 3 |
RbCrF5 (mp-645979) | 0.5054 | 0.041 | 3 |
SbTe(IF2)3 (mp-554942) | 0.6120 | 0.043 | 4 |
TeAs(IF2)3 (mp-555034) | 0.6219 | 0.084 | 4 |
ReSbOF9 (mp-541654) | 0.5930 | 0.024 | 4 |
Sb2SNF11 (mp-560450) | 0.4241 | 0.067 | 4 |
SbMoOF9 (mp-567264) | 0.4663 | 0.000 | 4 |
VF5 (mp-766781) | 0.3056 | 0.007 | 2 |
VF5 (mp-558797) | 0.4202 | 0.000 | 2 |
VF5 (mp-765273) | 0.3484 | 0.007 | 2 |
VF5 (mp-765241) | 0.4382 | 0.005 | 2 |
VF5 (mp-765218) | 0.3268 | 0.013 | 2 |
HgSb4C2(OF11)2 (mp-556903) | 0.5076 | 0.080 | 5 |
Sb4OsC6(O3F11)2 (mp-558754) | 0.6656 | 0.084 | 5 |
Sb2OsC4(OF3)4 (mp-559010) | 0.6507 | 0.057 | 5 |
Sb4RuC6(O3F11)2 (mp-555952) | 0.6650 | 0.092 | 5 |
FeSb4C6(O3F11)2 (mp-19590) | 0.6780 | 0.243 | 5 |
K3WC4N4OF (mp-651173) | 0.7473 | 0.255 | 6 |
Sb4IrC5ClO5F22 (mp-555612) | 0.6151 | 0.108 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv F |
Final Energy/Atom-5.2353 eV |
Corrected Energy-132.3761 eV
-132.3761 eV = -125.6481 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)