Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.800 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.082 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVO2 + LiF |
Band Gap1.636 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 1> | 209.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 293.4 |
CeO2 (mp-20194) | <1 1 1> | <1 0 1> | 251.5 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 137.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 123.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 74.0 |
AlN (mp-661) | <1 1 0> | <1 1 -1> | 141.8 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 222.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 148.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 203.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 228.8 |
GaN (mp-804) | <1 0 0> | <1 0 -1> | 191.9 |
GaN (mp-804) | <1 1 0> | <1 1 -1> | 141.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 269.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 284.6 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 230.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 152.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 -1> | 141.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 109.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 123.3 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 167.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 123.3 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 167.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 74.0 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 279.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 -1> | 246.7 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 274.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 125.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 209.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 271.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 284.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 230.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 308.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 222.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 305.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 192.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 137.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 228.8 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 230.7 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 167.7 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 335.4 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 154.0 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 269.5 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 228.8 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 209.6 |
CdS (mp-672) | <1 0 0> | <0 1 1> | 228.6 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 230.7 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 191.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 -1> | 137.0 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 230.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg2CuN2 (mvc-2126) | 0.4585 | 0.156 | 3 |
Mg2MnN2 (mvc-14629) | 0.5856 | 0.093 | 3 |
Ca2CuN2 (mvc-13711) | 0.5699 | 0.121 | 3 |
Li3V5O12 (mp-762254) | 0.5365 | 0.073 | 3 |
LiMnF3 (mp-763019) | 0.5964 | 0.078 | 3 |
Li2VO3F (mp-765755) | 0.5946 | 0.103 | 4 |
Li2Ti2FeO6 (mp-763753) | 0.6333 | 0.095 | 4 |
MgFeBiO5 (mvc-9221) | 0.6383 | 0.182 | 4 |
ZnNiBiO5 (mvc-9235) | 0.6501 | 0.177 | 4 |
Mg2MnWO6 (mvc-5930) | 0.6279 | 0.102 | 4 |
V4O7 (mp-715493) | 0.6796 | 0.274 | 2 |
Nb2O3 (mp-1095187) | 0.7329 | 0.081 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv O F |
Final Energy/Atom-6.0216 eV |
Corrected Energy-180.9521 eV
-180.9521 eV = -168.6058 eV (uncorrected energy) - 6.7280 eV (MP Advanced Correction) - 5.6183 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)