Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.136 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.066 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.32 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi5FeO4 + Li2O2 + LiF |
Band Gap0.228 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 307.3 |
AlN (mp-661) | <1 0 1> | <1 -1 1> | 106.5 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 260.1 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 325.2 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 184.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 307.3 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 197.3 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 260.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 260.1 |
AlN (mp-661) | <0 0 1> | <1 1 0> | 307.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 240.1 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 245.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 161.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 61.5 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 322.0 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 214.7 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 184.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 187.8 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 61.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 161.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 197.3 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 206.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 307.3 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 184.4 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 348.8 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 80.5 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 197.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 325.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 131.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 53.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 161.0 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 184.4 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 80.5 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 134.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 245.9 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 161.0 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 195.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 1> | 260.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 295.2 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 322.0 |
GaSe (mp-1943) | <0 0 1> | <1 1 1> | 263.0 |
BN (mp-984) | <0 0 1> | <1 1 0> | 245.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 322.0 |
MoS2 (mp-1434) | <1 1 0> | <1 1 0> | 122.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 80.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 161.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 245.9 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 134.2 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 322.0 |
BN (mp-984) | <1 0 0> | <0 0 1> | 348.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li9(NiO4)2 (mp-775731) | 0.4757 | 0.085 | 3 |
Li35(FeO4)8 (mp-853186) | 0.5346 | 0.043 | 3 |
Li9(FeO4)2 (mp-780203) | 0.5076 | 0.223 | 3 |
Li9(CoO4)2 (mp-776979) | 0.4662 | 0.078 | 3 |
Li4CoO4 (mp-763322) | 0.5650 | 0.168 | 3 |
Ca2YBiO5 (mvc-5445) | 0.5559 | 0.169 | 4 |
Ca2YSnO5 (mvc-6291) | 0.6143 | 0.182 | 4 |
Li7VO5F (mp-764210) | 0.1876 | 0.045 | 4 |
Li3MnO2F (mp-767306) | 0.5268 | 0.094 | 4 |
Li5WNO4 (mp-772397) | 0.6076 | 0.055 | 4 |
Al4C3 (mp-1591) | 0.6279 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Fe_pv O F |
Final Energy/Atom-5.1184 eV |
Corrected Energy-311.6084 eV
-311.6084 eV = -286.6306 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 10.9320 eV (MP Advanced Correction)
|