Final Magnetic Moment1.017 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.989 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.94 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiO2 + LiF |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [164] |
Hall-P 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 116.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 138.2 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 160.0 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 84.0 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 152.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 143.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 181.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 181.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 225.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 189.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 203.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 50.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 165.5 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 196.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 215.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 65.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 240.0 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 165.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 240.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 218.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 21.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 189.1 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 36.4 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 320.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 109.1 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 290.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 203.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 218.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 210.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 232.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 165.5 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 331.1 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 210.1 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 312.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 215.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.5 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 165.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 143.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 181.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 82.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 116.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 29.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 225.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 138.2 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 206.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 269.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 289.7 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 206.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 82.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiNiO2 (mp-25592) | 0.0861 | 0.012 | 3 |
YbTlS2 (mp-16472) | 0.1258 | 0.149 | 3 |
LiCuO2 (mp-25372) | 0.1012 | 0.068 | 3 |
LiMnO2 (mp-25539) | 0.1109 | 0.098 | 3 |
LiCoO2 (mp-894498) | 0.1173 | 0.032 | 3 |
Li4FeCu3O8 (mp-771812) | 0.0743 | 0.057 | 4 |
Li4CrFe3O8 (mp-769742) | 0.0765 | 1.512 | 4 |
Li4CrFe3O8 (mp-765495) | 0.0755 | 1.992 | 4 |
Li2MnO2F (mp-767107) | 0.0719 | 0.071 | 4 |
Li4TiCr3O8 (mp-765747) | 0.0689 | 0.235 | 4 |
Bi2Te3 (mp-568390) | 0.2113 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.2030 | 0.530 | 2 |
PbS (mp-1057015) | 0.2425 | 0.001 | 2 |
In2Se3 (mp-20830) | 0.1700 | 0.530 | 2 |
SrN (mp-1078609) | 0.2528 | 0.438 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6953 | 0.005 | 5 |
Hg (mp-982872) | 0.2850 | 0.020 | 1 |
Se (mp-7755) | 0.3299 | 0.181 | 1 |
Te (mp-10654) | 0.2820 | 0.047 | 1 |
Te (mp-105) | 0.3265 | 0.047 | 1 |
P (mp-53) | 0.3605 | 0.144 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv O F |
Final Energy/Atom-4.8800 eV |
Corrected Energy-65.6969 eV
-65.6969 eV = -58.5598 eV (uncorrected energy) - 4.3280 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)