Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.606 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.043 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn(PO3)2 + LiPO3 + NaPO3 |
Band Gap3.438 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 1 0> | 231.1 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 323.5 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 146.1 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 323.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 323.5 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 277.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 219.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 146.1 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 323.5 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 277.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 184.9 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 259.5 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 323.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 323.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 323.5 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 219.1 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 277.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 219.1 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 277.3 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 323.5 |
Ag (mp-124) | <1 0 0> | <1 1 -1> | 137.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 219.1 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 323.5 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 73.0 |
LiNbO3 (mp-3731) | <1 1 0> | <1 0 0> | 127.5 |
Al (mp-134) | <1 0 0> | <0 1 0> | 184.9 |
Al (mp-134) | <1 1 1> | <0 1 0> | 323.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 323.5 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 219.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 323.5 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 73.0 |
LiTaO3 (mp-3666) | <1 1 0> | <1 0 0> | 127.5 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 323.5 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 277.3 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 292.1 |
TiO2 (mp-2657) | <0 0 1> | <1 0 -1> | 129.8 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 292.1 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 231.1 |
TiO2 (mp-2657) | <1 1 1> | <0 1 0> | 231.1 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 1> | 168.7 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 219.1 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 146.1 |
C (mp-66) | <1 1 0> | <0 1 0> | 231.1 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 323.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 1 0> | 135.6 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 323.5 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 231.1 |
SiC (mp-11714) | <1 1 0> | <0 1 0> | 323.5 |
PbSe (mp-2201) | <1 1 0> | <0 1 0> | 277.3 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 323.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AgAsO3 (mp-558950) | 0.6413 | 0.026 | 3 |
Si2Sn2O7 (mp-769046) | 0.6191 | 0.086 | 3 |
Sn2Ge2O7 (mp-768877) | 0.6142 | 0.039 | 3 |
Mn5(P3O11)2 (mp-705036) | 0.6484 | 0.028 | 3 |
Co3(P2O7)2 (mp-540500) | 0.6522 | 0.025 | 3 |
Li2Mn(PO3)5 (mp-705355) | 0.5138 | 0.032 | 4 |
Na3Mg2P5O16 (mp-555005) | 0.5264 | 0.000 | 4 |
Na2Mn(PO3)5 (mp-567904) | 0.5099 | 0.000 | 4 |
LiNi(PO3)3 (mp-32400) | 0.5201 | 0.029 | 4 |
Na4Ca(PO3)6 (mp-542280) | 0.4452 | 0.000 | 4 |
Li2Mn2P2O7F2 (mp-770546) | 0.5952 | 0.098 | 5 |
LiVSO4F3 (mp-769601) | 0.5771 | 0.051 | 5 |
LiVSO4F3 (mp-768092) | 0.6298 | 0.057 | 5 |
LiVSO4F3 (mp-769603) | 0.5734 | 0.048 | 5 |
Na2ZrCo(P2O7)2 (mp-562673) | 0.5956 | 0.028 | 5 |
LiMnVP2(HO5)2 (mp-765378) | 0.6749 | 0.041 | 6 |
LiMnVP2(HO5)2 (mp-765074) | 0.6341 | 0.040 | 6 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.6615 | 0.000 | 6 |
LiMnVP2(HO5)2 (mp-765151) | 0.6969 | 0.042 | 6 |
LiMnVP2(HO5)2 (mp-765107) | 0.6882 | 0.042 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.6016 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Li_sv Mn_pv P O |
Final Energy/Atom-6.8884 eV |
Corrected Energy-355.0713 eV
-355.0713 eV = -330.6409 eV (uncorrected energy) - 21.0687 eV (MP Anion Correction) - 3.3617 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)