Final Magnetic Moment4.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.630 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.086 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.46 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO2 + MnF2 + LiF |
Band Gap1.042 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnn2 [34] |
HallP 2 2n |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 184.3 |
YVO4 (mp-19133) | <1 1 0> | <0 1 1> | 249.0 |
YVO4 (mp-19133) | <1 1 1> | <0 0 1> | 260.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 234.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 286.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 338.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 212.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 260.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 130.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 78.1 |
BN (mp-984) | <1 0 1> | <0 0 1> | 78.1 |
BN (mp-984) | <1 1 0> | <1 0 0> | 133.3 |
BN (mp-984) | <1 1 1> | <1 0 0> | 133.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 234.4 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 0> | 222.1 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 1> | 154.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 234.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 78.1 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 249.0 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 212.2 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 260.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 61.4 |
CeO2 (mp-20194) | <1 0 0> | <0 1 1> | 249.0 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 297.1 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 133.5 |
MoS2 (mp-1434) | <1 0 0> | <1 0 1> | 206.0 |
MoS2 (mp-1434) | <1 1 0> | <0 0 1> | 234.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 286.5 |
BaF2 (mp-1029) | <1 0 0> | <0 1 1> | 199.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 234.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 338.5 |
Al (mp-134) | <1 1 0> | <1 0 1> | 206.0 |
Al (mp-134) | <1 1 1> | <0 1 1> | 199.2 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 127.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 51.5 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 133.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 88.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 182.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 212.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 1> | 99.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 42.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 348.6 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 297.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 338.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 42.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 84.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 212.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 184.3 |
SiO2 (mp-6930) | <1 1 1> | <0 1 0> | 212.2 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 199.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiMnF3 (mp-765433) | 0.3912 | 0.029 | 3 |
LiFeO3 (mp-771612) | 0.3748 | 0.142 | 3 |
LiSbO3 (mp-4995) | 0.3933 | 0.000 | 3 |
LiVF3 (mp-777894) | 0.3933 | 0.028 | 3 |
Li3Fe5O12 (mp-773247) | 0.3677 | 0.141 | 3 |
Li3MnNb4O12 (mp-782651) | 0.3921 | 0.185 | 4 |
Li4Mn3TeO12 (mp-771455) | 0.3303 | 0.068 | 4 |
Li4Fe3TeO12 (mp-772725) | 0.2883 | 0.112 | 4 |
Li4Nb3TeO12 (mp-755915) | 0.3928 | 0.040 | 4 |
Li4Nb(FeO4)3 (mp-774238) | 0.3405 | 0.139 | 4 |
Fe2O3 (mp-777192) | 0.4433 | 0.732 | 2 |
Fe2O3 (mp-715276) | 0.5109 | 0.086 | 2 |
Al2O3 (mp-776490) | 0.5152 | 0.048 | 2 |
Cr3N2 (mp-1014444) | 0.5320 | 0.155 | 2 |
Mn2O3 (mp-565203) | 0.4804 | 0.000 | 2 |
Li4Fe2TeWO12 (mp-768021) | 0.4274 | 0.083 | 5 |
LaMgFeWO6 (mvc-9002) | 0.4767 | 0.079 | 5 |
LaMgFeSbO6 (mvc-9012) | 0.4877 | 0.220 | 5 |
Li4MnV2WO12 (mp-773239) | 0.4997 | 0.089 | 5 |
Li4V2CrTeO12 (mp-775632) | 0.4154 | 0.104 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv O F |
Final Energy/Atom-5.9252 eV |
Corrected Energy-128.0361 eV
-128.0361 eV = -118.5035 eV (uncorrected energy) - 6.7234 eV (MP Advanced Correction) - 2.8092 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)