Final Magnetic Moment0.212 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.612 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.064 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVPO5 + VP2O7 + Li6V3P8O29 + LiPO3 |
Band Gap0.009 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 248.0 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 136.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 165.4 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 136.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 136.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 82.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 248.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 136.5 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 248.0 |
Al (mp-134) | <1 1 0> | <0 1 0> | 136.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 82.7 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 165.4 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 165.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 248.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 248.0 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 165.4 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 248.0 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 165.4 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 248.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 248.0 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 165.4 |
NdGaO3 (mp-3196) | <0 1 1> | <0 0 1> | 165.4 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 248.0 |
C (mp-48) | <1 0 1> | <0 1 1> | 159.7 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 136.5 |
NaCl (mp-22862) | <1 1 0> | <0 1 0> | 136.5 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 165.4 |
Ge (mp-32) | <1 1 0> | <1 0 0> | 137.0 |
Al2O3 (mp-1143) | <0 0 1> | <0 1 1> | 159.7 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 248.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr3P4O15 (mp-763487) | 0.5231 | 0.087 | 3 |
Co5(P3O11)2 (mp-31617) | 0.5864 | 0.031 | 3 |
Cr(PO3)3 (mp-31690) | 0.5626 | 0.132 | 3 |
Ti7Cr12O48 (mp-853216) | 0.5888 | 0.091 | 3 |
Cr(PO3)3 (mp-694576) | 0.5713 | 0.132 | 3 |
Li4V3P8O29 (mp-765043) | 0.1708 | 0.053 | 4 |
Li4V3P8O29 (mp-765017) | 0.1681 | 0.061 | 4 |
Li5V3P8O29 (mp-774118) | 0.1381 | 0.088 | 4 |
Li4V3P8O29 (mp-851253) | 0.1724 | 0.046 | 4 |
Li4V3P8O29 (mp-763272) | 0.1786 | 0.057 | 4 |
Cr19O48 (mp-850874) | 0.5099 | 0.167 | 2 |
Cr19O48 (mp-780521) | 0.6215 | 0.085 | 2 |
Li3VSi4(HO6)2 (mp-770607) | 0.5794 | 0.030 | 5 |
LiSn2P4H3O16 (mp-754500) | 0.5731 | 0.061 | 5 |
LiVSO4F3 (mp-769603) | 0.6530 | 0.088 | 5 |
SnP4H8N2O13 (mp-603633) | 0.5104 | 0.010 | 5 |
TiP4H8N2O13 (mp-603612) | 0.6105 | 0.026 | 5 |
FeBP2H5NO9 (mp-766957) | 0.6614 | 0.100 | 6 |
VBP2H5NO9 (mp-25798) | 0.6316 | 0.000 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6578 | 0.041 | 6 |
Ca2MnAl2Si3HO13 (mp-745107) | 0.6596 | 0.075 | 6 |
NaMgAl3Si8(HO6)4 (mp-1094103) | 0.5848 | 0.025 | 6 |
Al2P2H8C2NO8F (mp-708964) | 0.7373 | 0.050 | 7 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7016 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.0155 eV |
Corrected Energy-681.4430 eV
Uncorrected energy = -631.3970 eV
Composition-based energy adjustment (-0.687 eV/atom x 58.0 atoms) = -39.8460 eV
Composition-based energy adjustment (-1.700 eV/atom x 6.0 atoms) = -10.2000 eV
Corrected energy = -681.4430 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)