Final Magnetic Moment38.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.352 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.771 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiFeO2 + Mn(FeO2)2 + LiMnO2 + Li2MnO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCc [9] |
HallC 2yc |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 158.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 138.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 138.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 138.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 180.7 |
BN (mp-984) | <1 0 1> | <0 1 0> | 180.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 138.5 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 271.1 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 271.1 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 138.5 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 271.1 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 158.3 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 158.3 |
Ga2O3 (mp-886) | <1 0 -1> | <0 1 0> | 271.1 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 138.5 |
C (mp-48) | <1 1 0> | <0 1 0> | 271.1 |
C (mp-48) | <1 1 1> | <0 1 0> | 271.1 |
ZrO2 (mp-2858) | <1 0 -1> | <0 1 0> | 180.7 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 271.1 |
TiO2 (mp-390) | <1 0 1> | <1 0 0> | 158.3 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 158.3 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 271.1 |
TiO2 (mp-390) | <1 1 1> | <0 1 0> | 271.1 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 138.5 |
Fe2O3 (mp-24972) | <0 0 1> | <0 0 1> | 138.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5(NiO2)8 (mp-762580) | 0.3813 | 0.131 | 3 |
Li6(NiO2)11 (mp-762450) | 0.3873 | 0.040 | 3 |
Li5Mn5O12 (mp-762417) | 0.3900 | 0.771 | 3 |
Li2Mn7O12 (mp-763611) | 0.3704 | 0.055 | 3 |
Li4Co5O12 (mp-868342) | 0.3844 | 0.118 | 3 |
Li2V5Cr2O12 (mp-782662) | 0.3797 | 0.153 | 4 |
Li2Ti2Mn5O12 (mp-762569) | 0.3620 | 0.091 | 4 |
Li3V2(O2F)2 (mp-764396) | 0.3781 | 0.057 | 4 |
Li2Mn5(FeO6)2 (mp-762813) | 0.3286 | 0.385 | 4 |
LiAlVO4 (mp-769572) | 0.3767 | 0.090 | 4 |
Ni3O4 (mp-714961) | 0.6029 | 0.000 | 2 |
Fe3O4 (mp-715614) | 0.5191 | 0.468 | 2 |
Fe3O4 (mp-612405) | 0.5536 | 0.876 | 2 |
Ni3O4 (mp-656887) | 0.5960 | 0.000 | 2 |
Zr3S4 (mp-684749) | 0.5561 | 0.000 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv Fe_pv O |
Final Energy/Atom-5.7518 eV |
Corrected Energy-460.9070 eV
Uncorrected energy = -402.6230 eV
Composition-based energy adjustment (-0.687 eV/atom x 36.0 atoms) = -24.7320 eV
Composition-based energy adjustment (-1.668 eV/atom x 12.0 atoms) = -20.0160 eV
Composition-based energy adjustment (-2.256 eV/atom x 6.0 atoms) = -13.5360 eV
Corrected energy = -460.9070 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)