Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.357 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnV2O6 + MnPH2O5 + Li3V2P4(HO8)2 + MnO2 |
Band Gap0.954 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 -1> | 247.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 217.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 178.4 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 217.0 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 229.6 |
GaAs (mp-2534) | <1 1 1> | <0 1 -1> | 293.5 |
GaN (mp-804) | <0 0 1> | <0 1 -1> | 293.5 |
GaN (mp-804) | <1 0 0> | <1 -1 0> | 285.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 229.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 217.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 237.9 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 289.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 -1> | 293.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 0> | 285.5 |
ZnSe (mp-1190) | <1 1 1> | <0 1 -1> | 293.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 297.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 -1> | 220.1 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 306.1 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 165.3 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 217.0 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 229.6 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 153.0 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 217.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 297.4 |
Te2W (mp-22693) | <1 1 1> | <0 1 -1> | 220.1 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 217.0 |
BN (mp-984) | <0 0 1> | <0 1 -1> | 146.8 |
BN (mp-984) | <1 0 1> | <1 0 0> | 306.1 |
Ag (mp-124) | <1 0 0> | <0 1 -1> | 293.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 217.0 |
MoS2 (mp-1434) | <0 0 1> | <0 1 -1> | 293.5 |
Al (mp-134) | <1 0 0> | <0 0 1> | 297.4 |
BN (mp-984) | <1 0 0> | <1 -1 -1> | 115.8 |
BN (mp-984) | <1 1 0> | <1 0 0> | 229.6 |
LiNbO3 (mp-3731) | <1 0 0> | <1 -1 1> | 217.0 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 217.0 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 -1> | 165.3 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 306.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 -1> | 293.5 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 297.4 |
TeO2 (mp-2125) | <1 1 0> | <0 1 -1> | 293.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 297.4 |
LiTaO3 (mp-3666) | <1 0 0> | <1 -1 1> | 217.0 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 178.4 |
TiO2 (mp-2657) | <1 0 0> | <0 1 -1> | 220.1 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 289.3 |
C (mp-66) | <1 0 0> | <0 1 0> | 217.0 |
C (mp-66) | <1 1 0> | <1 0 0> | 306.1 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 229.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 1 -1> | 293.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ni7(PO4)6 (mp-704235) | 0.6252 | 0.146 | 3 |
Mn2PO5 (mp-770540) | 0.6342 | 0.018 | 3 |
Cr5(PO4)4 (mp-540446) | 0.5994 | 0.007 | 3 |
Na2W2O7 (mp-25800) | 0.6158 | 0.022 | 3 |
Cr5(PO4)4 (mp-775246) | 0.6118 | 0.007 | 3 |
Li2Fe(PO4)2 (mp-697816) | 0.5205 | 0.083 | 4 |
Li2Mn2(SO4)3 (mp-770262) | 0.5081 | 0.013 | 4 |
LiNi(SO4)2 (mp-775498) | 0.5153 | 0.043 | 4 |
Li2Cr(PO4)2 (mp-540343) | 0.5334 | 0.062 | 4 |
Li2V2(SO4)3 (mp-566770) | 0.5194 | 0.043 | 4 |
Cr5O12 (mp-19575) | 0.7356 | 0.025 | 2 |
Li7CrFe3(PO4)6 (mp-765435) | 0.5256 | 0.452 | 5 |
Li7Cr3Co(PO4)6 (mp-780115) | 0.5087 | 0.075 | 5 |
Li7Cr3Fe(PO4)6 (mp-780107) | 0.5253 | 0.208 | 5 |
Li7Fe3Ni(PO4)6 (mp-775193) | 0.5008 | 0.043 | 5 |
Li2MnV(PO4)3 (mp-779088) | 0.5217 | 0.031 | 5 |
LiMnVP2(HO5)2 (mp-765074) | 0.1467 | 0.040 | 6 |
LiMnVP2(HO5)2 (mp-765151) | 0.1310 | 0.042 | 6 |
LiVCrP2(HO5)2 (mp-765109) | 0.1448 | 0.016 | 6 |
LiMnVP2(HO5)2 (mp-765103) | 0.1301 | 0.039 | 6 |
LiVCrP2(HO5)2 (mp-765072) | 0.1500 | 0.014 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7124 | 0.002 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv P H O |
Final Energy/Atom-6.8599 eV |
Corrected Energy-381.0141 eV
-381.0141 eV = -349.8568 eV (uncorrected energy) - 21.0687 eV (MP Anion Correction) - 10.0886 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)