Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.928 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.078 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCoCO3 + Li2CO3 |
Band Gap2.137 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFdd2 [43] |
HallF 2 2d |
Point Groupmm2 |
Crystal Systemorthorhombic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 175.5 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 235.7 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 263.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 176.8 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 294.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 190.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 190.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 87.7 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 1> | 105.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 263.2 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 175.5 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 263.2 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 294.6 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 1> | 211.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 294.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 58.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 211.4 |
BN (mp-984) | <0 0 1> | <0 0 1> | 235.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 294.6 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 117.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 58.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 180.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 176.8 |
Al (mp-134) | <1 0 0> | <0 1 0> | 263.2 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 294.6 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 105.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 87.7 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 263.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 263.2 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 263.2 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 294.6 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 294.6 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 235.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 190.0 |
GdScO3 (mp-5690) | <0 1 0> | <0 0 1> | 176.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 263.2 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 176.8 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 58.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 235.7 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 58.9 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 176.8 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 87.7 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 0> | 263.2 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 176.8 |
Si (mp-149) | <1 0 0> | <0 0 1> | 58.9 |
Si (mp-149) | <1 1 0> | <0 1 1> | 211.4 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 58.9 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 117.9 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 294.6 |
SiC (mp-8062) | <1 1 1> | <0 0 1> | 235.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2CrN3 (mvc-11104) | 0.6959 | 0.480 | 3 |
Ca2VN3 (mvc-10945) | 0.7372 | 0.708 | 3 |
Ag2CO3 (mp-676581) | 0.7319 | 0.029 | 3 |
Rb3FeO3 (mp-770126) | 0.7108 | 0.107 | 3 |
Li2Fe(CO3)2 (mp-762005) | 0.6241 | 0.052 | 4 |
Li2Ni(CO3)2 (mp-763387) | 0.3357 | 0.088 | 4 |
Li2Cr(CO3)2 (mp-768000) | 0.2489 | 0.068 | 4 |
Li6Cr(BO3)3 (mp-772644) | 0.5937 | 0.079 | 4 |
Li6Mn(BO3)3 (mp-772526) | 0.6073 | 0.057 | 4 |
Li4Mn2Fe(BO3)4 (mp-767650) | 0.7498 | 0.069 | 5 |
LiCuHCO4 (mp-769201) | 0.6658 | 0.094 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co C O |
Final Energy/Atom-6.7370 eV |
Corrected Energy-160.3903 eV
-160.3903 eV = -148.2148 eV (uncorrected energy) - 8.4275 eV (MP Anion Correction) - 3.7480 eV (MP Advanced Correction)
|