Final Magnetic Moment3.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.667 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.048 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.59 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6V3P8O29 |
Band Gap1.347 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 250.5 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 136.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 136.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 167.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 250.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 136.5 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 136.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 83.5 |
BN (mp-984) | <1 0 1> | <1 -1 1> | 160.4 |
Al (mp-134) | <1 1 0> | <0 1 0> | 136.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 83.5 |
C (mp-66) | <1 1 0> | <0 0 1> | 250.5 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 167.0 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 136.5 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 167.0 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 250.5 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 250.5 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 136.5 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 167.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 83.5 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 167.0 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 136.5 |
C (mp-48) | <1 0 1> | <1 -1 1> | 160.4 |
NaCl (mp-22862) | <1 1 0> | <0 1 0> | 136.5 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 83.5 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 167.0 |
Ge (mp-32) | <1 1 0> | <1 0 0> | 136.8 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 1> | 160.3 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 250.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn7Cr12O48 (mp-774029) | 0.6634 | 0.078 | 3 |
Ti7Cr12O48 (mp-853216) | 0.5406 | 0.084 | 3 |
Fe2(WO4)3 (mvc-8014) | 0.6029 | 0.124 | 3 |
Fe2(MoO4)3 (mvc-8023) | 0.5945 | 0.047 | 3 |
Cr3(FeO6)2 (mvc-7922) | 0.6395 | 0.031 | 3 |
Li6V3P8O29 (mp-761507) | 0.1151 | 0.049 | 4 |
Li6V3P8O29 (mp-761498) | 0.1202 | 0.049 | 4 |
Li6V3P8O29 (mp-773609) | 0.1209 | 0.046 | 4 |
Li6V3P8O29 (mp-773379) | 0.0950 | 0.048 | 4 |
Li6V3P8O29 (mp-763866) | 0.1188 | 0.048 | 4 |
Cr19O48 (mp-850874) | 0.5392 | 0.097 | 2 |
Cr19O48 (mp-780521) | 0.6142 | 0.085 | 2 |
FeP3H5NO10 (mp-743646) | 0.6503 | 0.000 | 5 |
LiSn2P4H3O16 (mp-759095) | 0.6186 | 0.041 | 5 |
LiSn2P4H3O16 (mp-754500) | 0.6395 | 0.059 | 5 |
TeP2H16N2O13 (mp-707772) | 0.6318 | 0.045 | 5 |
SnP4H8N2O13 (mp-603633) | 0.6490 | 0.010 | 5 |
Ti2P4H9C2NO16 (mp-709069) | 0.6206 | 0.039 | 6 |
VBP2H5NO9 (mp-25798) | 0.7084 | 0.000 | 6 |
Al3P3H9C3NO14 (mp-699455) | 0.7378 | 0.065 | 6 |
AlBP2H5NO9 (mp-24757) | 0.7270 | 0.000 | 6 |
NaMgAl3Si8(HO6)4 (mp-1094103) | 0.7482 | 0.027 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.0172 eV |
Corrected Energy-696.4081 eV
-696.4081 eV = -645.5832 eV (uncorrected energy) - 40.7328 eV (MP Anion Correction) - 10.0920 eV (MP Advanced Correction)
|