Final Magnetic Moment15.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.350 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.089 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTe3P2O11 + CrPO4 + Cr(PO3)3 + Mn2P2O7 + Te |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 261.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 195.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 190.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 326.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 195.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 195.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 195.8 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 261.0 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 261.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 261.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 261.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 65.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 65.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 195.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 326.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 195.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 65.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 65.3 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 326.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 195.8 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 130.5 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 195.8 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 261.0 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 65.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 195.8 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 326.3 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 195.8 |
C (mp-66) | <1 1 1> | <0 0 1> | 65.3 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 326.3 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 326.3 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 261.0 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 65.3 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 326.3 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 261.0 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 65.3 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 261.0 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 65.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 195.8 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 65.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 195.8 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 261.0 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 261.0 |
Si (mp-149) | <1 1 0> | <0 0 1> | 326.3 |
Si (mp-149) | <1 1 1> | <0 0 1> | 195.8 |
Au (mp-81) | <1 1 1> | <0 0 1> | 261.0 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 195.8 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 65.3 |
C (mp-48) | <0 0 1> | <0 0 1> | 195.8 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 195.8 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 261.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.3014 | 0.050 | 3 |
VPO4 (mp-861584) | 0.3633 | 0.076 | 3 |
MnPO4 (mp-504382) | 0.4611 | 0.070 | 3 |
Cr3AgO8 (mp-560237) | 0.4757 | 0.000 | 3 |
TiPO4 (mp-779587) | 0.4605 | 0.077 | 3 |
Mn5Fe(PO4)6 (mp-772374) | 0.2629 | 0.040 | 4 |
TiMn5(PO4)6 (mp-772326) | 0.2653 | 0.037 | 4 |
V2Sb(PO4)3 (mp-773573) | 0.2381 | 0.085 | 4 |
Mn5V(PO4)6 (mp-773464) | 0.2656 | 0.038 | 4 |
Mn5Sb(PO4)6 (mp-773395) | 0.2535 | 0.041 | 4 |
CrFe3Sb2(PO4)6 (mp-775989) | 0.1803 | 0.032 | 5 |
VFe3Sb2(PO4)6 (mp-761422) | 0.1738 | 0.049 | 5 |
V3FeSb2(PO4)6 (mp-762598) | 0.1697 | 0.074 | 5 |
CrFe3Sn2(PO4)6 (mp-776666) | 0.1816 | 0.082 | 5 |
Cr3NiTe2(PO4)6 (mp-765190) | 0.1397 | 0.085 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.4474 | 0.065 | 6 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.4156 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.3406 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.4653 | 0.015 | 6 |
Na2LiTi3Al(PO4)6 (mp-769073) | 0.4732 | 0.014 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVCr: 3.7 eV |
PseudopotentialsVASP PAW: Mn_pv Cr_pv Te P O |
Final Energy/Atom-7.1021 eV |
Corrected Energy-280.2519 eV
-280.2519 eV = -255.6771 eV (uncorrected energy) - 16.8550 eV (MP Anion Correction) - 7.7199 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)