Final Magnetic Moment0.030 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.610 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.065 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVPO5 + VP2O7 + Li6V3P8O29 + LiPO3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 249.1 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 136.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 249.1 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 136.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 166.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 136.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 136.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 83.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 249.1 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 249.1 |
Al (mp-134) | <1 1 0> | <0 1 0> | 136.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 83.0 |
TbScO3 (mp-31119) | <1 0 0> | <0 1 0> | 136.8 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 166.1 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 249.1 |
C (mp-48) | <1 0 1> | <0 1 1> | 159.8 |
Al2O3 (mp-1143) | <0 0 1> | <0 1 1> | 159.8 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 166.1 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 0> | 136.8 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 166.1 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 249.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 249.1 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 166.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 249.1 |
WS2 (mp-224) | <1 0 0> | <0 1 0> | 136.8 |
NaCl (mp-22862) | <1 1 0> | <0 1 0> | 136.8 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 166.1 |
Ge (mp-32) | <1 1 0> | <0 1 0> | 136.8 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 249.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr3P4O15 (mp-763487) | 0.5571 | 0.087 | 3 |
Mn7Cr12O48 (mp-774029) | 0.5917 | 0.078 | 3 |
Cr(PO3)3 (mp-31690) | 0.6006 | 0.132 | 3 |
Ti7Cr12O48 (mp-853216) | 0.5554 | 0.091 | 3 |
Cr(PO3)3 (mp-694576) | 0.6085 | 0.132 | 3 |
Li5V3P8O29 (mp-775505) | 0.1043 | 0.071 | 4 |
Li5V3P8O29 (mp-775385) | 0.0896 | 0.073 | 4 |
Li5V3P8O29 (mp-766628) | 0.1205 | 0.067 | 4 |
Li5V3P8O29 (mp-851057) | 0.1340 | 0.070 | 4 |
Li5V3P8O29 (mp-765155) | 0.1283 | 0.057 | 4 |
Cr19O48 (mp-850874) | 0.5108 | 0.167 | 2 |
Cr19O48 (mp-780521) | 0.5918 | 0.085 | 2 |
Cr5O12 (mp-19575) | 0.7449 | 0.142 | 2 |
Li3VSi4(HO6)2 (mp-770607) | 0.6519 | 0.030 | 5 |
LiSn2P4H3O16 (mp-754500) | 0.6415 | 0.061 | 5 |
TeP2H16N2O13 (mp-707772) | 0.6779 | 0.045 | 5 |
SnP4H8N2O13 (mp-603633) | 0.5586 | 0.010 | 5 |
TiP4H8N2O13 (mp-603612) | 0.6589 | 0.026 | 5 |
FeBP2H5NO9 (mp-766957) | 0.6668 | 0.100 | 6 |
VBP2H5NO9 (mp-25798) | 0.6276 | 0.000 | 6 |
Li2MgCr3Se3(SO8)3 (mp-773983) | 0.6654 | 0.041 | 6 |
AlBP2H5NO9 (mp-24757) | 0.6655 | 0.000 | 6 |
NaMgAl3Si8(HO6)4 (mp-1094103) | 0.6107 | 0.025 | 6 |
Al2P2H8C2NO8F (mp-708964) | 0.7300 | 0.050 | 7 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7406 | 0.068 | 7 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P O |
Final Energy/Atom-7.0142 eV |
Corrected Energy-681.3250 eV
Uncorrected energy = -631.2790 eV
Composition-based energy adjustment (-0.687 eV/atom x 58.0 atoms) = -39.8460 eV
Composition-based energy adjustment (-1.700 eV/atom x 6.0 atoms) = -10.2000 eV
Corrected energy = -681.3250 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)