Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-2.814 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.013 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.66 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVF5 |
Band Gap2.996 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 -1> | 234.7 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 194.6 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 295.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 197.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 344.8 |
GaN (mp-804) | <1 1 1> | <1 1 -1> | 152.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 197.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 253.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 246.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 295.5 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 218.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 344.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 197.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 344.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 197.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 197.0 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 253.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 344.8 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 197.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 295.5 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 246.3 |
Al (mp-134) | <1 1 0> | <0 0 1> | 344.8 |
Al (mp-134) | <1 1 1> | <0 0 1> | 197.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 253.3 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 147.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 49.3 |
SiC (mp-7631) | <1 1 0> | <1 0 -1> | 234.7 |
MgO (mp-1265) | <1 0 0> | <1 0 -1> | 234.7 |
MgO (mp-1265) | <1 1 0> | <1 0 -1> | 234.7 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 344.8 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 194.6 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 98.5 |
C (mp-66) | <1 1 1> | <0 0 1> | 197.0 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 111.7 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 197.0 |
TbScO3 (mp-31119) | <1 1 1> | <0 0 1> | 147.8 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 197.0 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 223.4 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 344.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 344.8 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 344.8 |
MoSe2 (mp-1634) | <1 0 0> | <1 1 -1> | 152.5 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 0> | 292.0 |
Au (mp-81) | <1 0 0> | <1 0 0> | 223.4 |
Au (mp-81) | <1 1 1> | <0 0 1> | 344.8 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 197.0 |
C (mp-48) | <0 0 1> | <1 0 1> | 126.6 |
C (mp-48) | <1 0 0> | <0 0 1> | 344.8 |
C (mp-48) | <1 0 1> | <0 0 1> | 246.3 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 344.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba2Ti2CuF14 (mvc-1612) | 0.5932 | 0.048 | 4 |
RbMoIO6 (mp-568192) | 0.5840 | 0.000 | 4 |
KY(WO4)2 (mp-510264) | 0.5664 | 0.000 | 4 |
KEr(WO4)2 (mp-566132) | 0.5709 | 0.000 | 4 |
Cs2KMn3F12 (mp-619127) | 0.5450 | 0.000 | 4 |
VF5 (mp-765273) | 0.3125 | 0.007 | 2 |
CrF5 (mp-639662) | 0.6090 | 0.000 | 2 |
VF4 (mp-765239) | 0.5973 | 0.056 | 2 |
Sb7F29 (mp-29369) | 0.6088 | 0.000 | 2 |
SeBr4 (mp-651332) | 0.4901 | 0.000 | 2 |
Sb2Cl5F4 (mp-680240) | 0.5624 | 0.000 | 3 |
Sb2TeF14 (mp-27473) | 0.5612 | 0.000 | 3 |
Sb2XeF14 (mp-27290) | 0.5479 | 0.000 | 3 |
OsOF4 (mp-558879) | 0.5165 | 0.016 | 3 |
SbOF3 (mp-757111) | 0.4214 | 0.009 | 3 |
TiTlWO5F (mp-690560) | 0.5938 | 0.000 | 5 |
TiNbTl(O2F)2 (mp-677378) | 0.7258 | 0.030 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-points16 |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv F |
Final Energy/Atom-5.2309 eV |
Corrected Energy-264.5389 eV
-264.5389 eV = -251.0829 eV (uncorrected energy) - 13.4560 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)