Final Magnetic Moment4.391 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.013 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.075 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.54 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi2Ti3VO8 + LiTi2O4 + Li2TiO3 + V |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <1 1 0> | 280.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 206.7 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 275.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 275.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 206.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 280.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.9 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 206.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 275.5 |
InAs (mp-20305) | <1 0 0> | <1 1 1> | 114.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 275.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.9 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 206.7 |
BN (mp-984) | <1 1 1> | <1 1 0> | 280.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 68.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 206.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 275.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 275.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 68.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 280.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 1> | 229.1 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 278.3 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 278.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 68.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 275.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 275.5 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 206.7 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 206.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 0> | 279.0 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 206.7 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 68.9 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 278.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 275.5 |
Ni (mp-23) | <1 0 0> | <1 1 0> | 186.7 |
PbSe (mp-2201) | <1 0 0> | <1 1 1> | 114.5 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 275.5 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 68.9 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 279.0 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 206.7 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 278.3 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 275.5 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 206.7 |
SiC (mp-11714) | <1 1 0> | <1 1 0> | 280.1 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 275.5 |
MoSe2 (mp-1634) | <1 1 1> | <0 0 1> | 275.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 275.5 |
Si (mp-149) | <1 1 1> | <0 0 1> | 206.7 |
Au (mp-81) | <1 1 1> | <0 0 1> | 206.7 |
CdSe (mp-2691) | <1 0 0> | <1 1 1> | 114.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiTi2O4 (mp-760832) | 0.4946 | 0.096 | 3 |
LiMn2O4 (mp-762459) | 0.3866 | 0.056 | 3 |
Li6(NiO2)11 (mp-762450) | 0.4974 | 0.040 | 3 |
Li5Mn5O12 (mp-762417) | 0.4267 | 0.771 | 3 |
Li2Mn7O12 (mp-763611) | 0.3948 | 0.055 | 3 |
Li2Ti2Mn5O12 (mp-762569) | 0.4327 | 0.091 | 4 |
Li3Mn2(CoO4)2 (mp-766797) | 0.4238 | 0.193 | 4 |
Li3Fe2Co3O10 (mp-763770) | 0.3666 | 0.209 | 4 |
Li6Fe3Co7O20 (mp-763066) | 0.4407 | 0.060 | 4 |
Li8Mn6(FeO6)3 (mp-765100) | 0.4227 | 0.771 | 4 |
Ni3O4 (mp-714961) | 0.7180 | 0.000 | 2 |
Fe3O4 (mp-715614) | 0.5845 | 0.468 | 2 |
Fe3O4 (mp-612405) | 0.6023 | 0.876 | 2 |
Ni3O4 (mp-849536) | 0.6695 | 0.130 | 2 |
Ni3Cl4 (mp-1096769) | 0.7197 | 0.045 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv Ti_pv V_pv O |
Final Energy/Atom-7.8069 eV |
Corrected Energy-545.0856 eV
Uncorrected energy = -515.2536 eV
Composition-based energy adjustment (-0.687 eV/atom x 36.0 atoms) = -24.7320 eV
Composition-based energy adjustment (-1.700 eV/atom x 3.0 atoms) = -5.1000 eV
Corrected energy = -545.0856 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)