Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.408 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.071 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiSnPO4 |
Band Gap3.300 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 200.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 -1> | 194.5 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 134.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 133.8 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 267.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 200.7 |
CdTe (mp-406) | <1 1 1> | <0 1 0> | 155.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 -1> | 116.5 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 200.7 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 66.9 |
TePb (mp-19717) | <1 1 1> | <0 1 0> | 155.7 |
Ag (mp-124) | <1 1 0> | <1 1 -1> | 194.5 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 155.7 |
TiO2 (mp-2657) | <1 1 0> | <1 0 -1> | 116.5 |
Al (mp-134) | <1 0 0> | <1 1 -1> | 194.5 |
TeO2 (mp-2125) | <0 0 1> | <1 1 -1> | 194.5 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 -1> | 233.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 -1> | 233.1 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 267.7 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 134.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 267.7 |
Ni (mp-23) | <1 0 0> | <1 0 -1> | 233.1 |
InSb (mp-20012) | <1 1 1> | <0 1 0> | 155.7 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 267.7 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 0> | 155.7 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 155.7 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 267.7 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 133.8 |
WS2 (mp-224) | <1 1 0> | <1 0 -1> | 233.1 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 200.7 |
TiO2 (mp-390) | <1 1 0> | <0 1 0> | 155.7 |
MgAl2O4 (mp-3536) | <1 1 0> | <1 1 -1> | 194.5 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 267.7 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 200.7 |
MgF2 (mp-1249) | <1 0 1> | <1 0 -1> | 233.1 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 267.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Bi6P2O15 (mp-767410) | 0.5090 | 0.072 | 3 |
Sn8P2O13 (mp-767039) | 0.4079 | 0.025 | 3 |
P2Pb4O9 (mp-31068) | 0.4969 | 0.000 | 3 |
As2Pb8O13 (mp-31107) | 0.4500 | 0.000 | 3 |
MoPb5O8 (mp-652366) | 0.4558 | 0.012 | 3 |
LiNiPO4 (mp-765389) | 0.5085 | 0.084 | 4 |
Li2CuP2O7 (mp-758486) | 0.5549 | 0.070 | 4 |
LiMnPO4 (mp-761562) | 0.5251 | 0.078 | 4 |
LiSnPO4 (mp-757042) | 0.4716 | 0.062 | 4 |
Rb3NaTiO4 (mp-560476) | 0.5516 | 0.000 | 4 |
K2LiVPO6 (mp-764301) | 0.6514 | 0.080 | 5 |
Li2FeP2HO8 (mp-705456) | 0.6779 | 0.305 | 5 |
Sr2YAlW2O7 (mvc-356) | 0.5995 | 0.551 | 5 |
Na2Al2Si3(HO3)4 (mp-510599) | 0.6795 | 0.565 | 5 |
Li2SbSO4F3 (mp-769153) | 0.6561 | 0.069 | 5 |
Na2LiCaVP2O9 (mp-763838) | 0.6621 | 0.111 | 6 |
LiPH4NO3F (mp-720554) | 0.7243 | 0.015 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv Sn_d P O |
Final Energy/Atom-6.4534 eV |
Corrected Energy-575.7941 eV
-575.7941 eV = -542.0842 eV (uncorrected energy) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)