Final Magnetic Moment0.479 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.224 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.154 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.11 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV4Fe2O13 + FePO4 + Li3V2P4(HO8)2 + Fe4P3(HO5)3 + H2O |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 272.8 |
CeO2 (mp-20194) | <1 0 0> | <1 -1 1> | 246.8 |
GaAs (mp-2534) | <1 0 0> | <0 1 1> | 299.4 |
BaF2 (mp-1029) | <1 0 0> | <0 1 -1> | 274.6 |
GaN (mp-804) | <0 0 1> | <1 -1 -1> | 248.5 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 218.2 |
GaN (mp-804) | <1 1 1> | <1 -1 1> | 246.8 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 149.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 255.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 -1 -1> | 165.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 274.6 |
AlN (mp-661) | <1 0 1> | <1 -1 1> | 246.8 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 273.0 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 228.2 |
LiF (mp-1138) | <1 0 0> | <1 1 1> | 251.0 |
Te2W (mp-22693) | <0 0 1> | <0 1 1> | 224.6 |
Te2W (mp-22693) | <1 1 1> | <0 1 1> | 224.6 |
GaN (mp-804) | <1 0 1> | <0 1 -1> | 329.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 146.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 224.6 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 272.8 |
YVO4 (mp-19133) | <1 1 1> | <1 1 1> | 251.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 273.0 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 251.0 |
InAs (mp-20305) | <1 0 0> | <0 1 -1> | 274.6 |
ZnSe (mp-1190) | <1 0 0> | <0 1 1> | 299.4 |
Ag (mp-124) | <1 0 0> | <1 0 1> | 273.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 255.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 299.4 |
CdS (mp-672) | <0 0 1> | <1 -1 1> | 246.8 |
CdS (mp-672) | <1 1 0> | <0 1 -1> | 329.5 |
CdS (mp-672) | <1 1 1> | <1 -1 1> | 164.5 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 292.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 219.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 328.7 |
GaSe (mp-1943) | <1 0 0> | <0 1 0> | 272.8 |
GaSe (mp-1943) | <1 0 1> | <1 0 1> | 273.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 182.6 |
BN (mp-984) | <1 0 0> | <0 1 0> | 272.8 |
BN (mp-984) | <1 0 1> | <0 0 1> | 182.6 |
BN (mp-984) | <1 1 0> | <0 0 1> | 292.2 |
Al (mp-134) | <1 0 0> | <0 1 -1> | 274.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 218.2 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 226.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 255.7 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 73.0 |
TeO2 (mp-2125) | <0 0 1> | <0 1 1> | 299.4 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 -1 1> | 246.8 |
MoS2 (mp-1434) | <0 0 1> | <1 -1 1> | 246.8 |
MoS2 (mp-1434) | <1 0 1> | <0 1 -1> | 274.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn2PO5 (mp-770540) | 0.6067 | 0.018 | 3 |
Mn7(PO4)6 (mp-770696) | 0.5825 | 0.010 | 3 |
Cr5(PO4)4 (mp-540446) | 0.5890 | 0.007 | 3 |
Na2W2O7 (mp-25800) | 0.6168 | 0.021 | 3 |
Cr5(PO4)4 (mp-775246) | 0.5964 | 0.007 | 3 |
Li2Fe(PO4)2 (mp-697816) | 0.4767 | 0.181 | 4 |
Li2Mn2(SO4)3 (mp-770262) | 0.4868 | 0.013 | 4 |
LiPWO5 (mp-763520) | 0.4920 | 0.035 | 4 |
Li2V2(SO4)3 (mp-566770) | 0.4816 | 0.127 | 4 |
Li2Ni(PO4)2 (mp-704224) | 0.5033 | 0.200 | 4 |
LiVPHO5 (mp-767213) | 0.5268 | 0.000 | 5 |
LiSbPHO5 (mp-755185) | 0.5484 | 0.076 | 5 |
Li7Cr3Co(PO4)6 (mp-780115) | 0.5025 | 0.105 | 5 |
Li7Fe3Ni(PO4)6 (mp-775193) | 0.5056 | 0.039 | 5 |
LiNiPO4F (mp-504104) | 0.5304 | 0.099 | 5 |
LiVFeP2(HO5)2 (mp-767445) | 0.1594 | 0.020 | 6 |
LiVFeP2(HO5)2 (mp-765318) | 0.1494 | 0.240 | 6 |
LiVCrP2(HO5)2 (mp-765112) | 0.1268 | 0.124 | 6 |
LiVFeP2(HO5)2 (mp-765111) | 0.1541 | 0.237 | 6 |
LiVFeP2(HO5)2 (mp-765075) | 0.1490 | 0.240 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eVFe: 5.3 eV |
PseudopotentialsVASP PAW: Li_sv V_pv Fe_pv P H O |
Final Energy/Atom-6.6242 eV |
Corrected Energy-248.0987 eV
-248.0987 eV = -225.2229 eV (uncorrected energy) - 14.0458 eV (MP Anion Correction) - 8.8300 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)