Final Magnetic Moment14.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.994 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.076 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVF2 + VF3 |
Band Gap0.644 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiC (mp-7631) | <0 0 1> | <0 1 0> | 272.9 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 204.7 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 237.0 |
Mg (mp-153) | <1 0 1> | <0 1 0> | 204.7 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 158.5 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 68.2 |
PbS (mp-21276) | <1 1 0> | <1 0 -1> | 248.1 |
PbS (mp-21276) | <1 1 1> | <1 0 -1> | 124.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 272.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 237.0 |
GaP (mp-2490) | <1 0 0> | <0 1 0> | 272.9 |
InP (mp-20351) | <1 1 0> | <1 0 -1> | 248.1 |
InP (mp-20351) | <1 1 1> | <1 0 -1> | 124.1 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 237.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 237.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 237.0 |
BaTiO3 (mp-5986) | <0 0 1> | <0 1 0> | 272.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 272.9 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 272.9 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 272.9 |
BN (mp-984) | <1 0 0> | <0 1 0> | 136.5 |
BN (mp-984) | <1 0 1> | <0 1 0> | 204.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 237.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 124.1 |
Al (mp-134) | <1 0 0> | <0 1 0> | 272.9 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 272.9 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 272.9 |
MoSe2 (mp-1634) | <1 1 0> | <0 1 0> | 272.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 272.9 |
Si (mp-149) | <1 0 0> | <0 1 0> | 272.9 |
WS2 (mp-224) | <0 0 1> | <1 0 -1> | 124.1 |
WS2 (mp-224) | <1 0 1> | <0 0 1> | 237.0 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 158.5 |
WS2 (mp-224) | <1 1 1> | <1 0 -1> | 248.1 |
C (mp-48) | <1 0 1> | <0 1 0> | 136.5 |
C (mp-48) | <1 1 1> | <0 0 1> | 237.0 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 237.0 |
ZrO2 (mp-2858) | <1 0 0> | <1 1 0> | 172.5 |
ZrO2 (mp-2858) | <1 0 1> | <1 1 0> | 172.5 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 158.5 |
YAlO3 (mp-3792) | <1 1 0> | <1 1 0> | 172.5 |
TiO2 (mp-390) | <0 0 1> | <1 1 0> | 172.5 |
Ge (mp-32) | <1 1 0> | <0 0 1> | 237.0 |
CaF2 (mp-2741) | <1 0 0> | <0 1 0> | 272.9 |
CdWO4 (mp-19387) | <1 1 0> | <0 1 0> | 204.7 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 272.9 |
SrTiO3 (mp-4651) | <0 0 1> | <0 1 0> | 272.9 |
Cu (mp-30) | <1 0 0> | <0 1 0> | 272.9 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 118.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv F |
Final Energy/Atom-6.2830 eV |
Corrected Energy-435.7523 eV
-435.7523 eV = -402.1123 eV (uncorrected energy) - 33.6400 eV (MP Advanced Correction)
|