Final Magnetic Moment25.012 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.278 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.058 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.92 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi6MnO4 + MnO + LiCrO2 + LiVO2 |
Band Gap1.817 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 221.2 |
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 284.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 221.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 347.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 126.4 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 158.0 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 221.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 221.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 284.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 221.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 181.2 |
GaN (mp-804) | <1 0 1> | <1 -1 1> | 204.9 |
GaN (mp-804) | <1 1 0> | <0 1 1> | 272.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 284.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 221.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 1> | 272.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.6 |
InAs (mp-20305) | <1 1 0> | <1 -1 1> | 273.2 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 221.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 239.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 208.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 284.4 |
CdS (mp-672) | <1 0 0> | <1 -1 1> | 204.9 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 302.1 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 299.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 252.8 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 208.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 347.6 |
YVO4 (mp-19133) | <0 0 1> | <1 1 0> | 104.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 221.2 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 179.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 158.0 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 126.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 31.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 221.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 284.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 221.2 |
BN (mp-984) | <1 1 0> | <0 1 0> | 239.9 |
BN (mp-984) | <1 1 1> | <0 1 0> | 299.9 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 94.8 |
Al (mp-134) | <1 0 0> | <0 1 0> | 239.9 |
Al (mp-134) | <1 1 0> | <1 1 0> | 208.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 221.2 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 347.6 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 347.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 221.2 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 181.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 94.8 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 284.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 158.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li5(NiO2)4 (mp-780518) | 0.4346 | 0.327 | 3 |
Li5(FeO2)4 (mp-780312) | 0.2736 | 0.259 | 3 |
Li5(CoO2)4 (mp-780140) | 0.2073 | 0.228 | 3 |
Li5Cr4O8 (mp-850237) | 0.3187 | 0.101 | 3 |
Li5Mn4O8 (mp-849676) | 0.5855 | 0.966 | 3 |
Li10Mn5Fe3O16 (mp-765033) | 0.2077 | 0.072 | 4 |
Li5Cr3NiO8 (mp-764311) | 0.1939 | 0.279 | 4 |
Li10V5Cr3O16 (mp-764037) | 0.1917 | 0.081 | 4 |
Li5VCr3O8 (mp-765717) | 0.2134 | 0.084 | 4 |
Li5MnCr3O8 (mp-765322) | 0.1306 | 0.063 | 4 |
Ti3N4 (mp-1080192) | 0.7381 | 0.100 | 2 |
Li10Mn2Fe3Ni3O16 (mp-764933) | 0.2750 | 0.079 | 5 |
Li10Mn3Cr3(CoO8)2 (mp-780494) | 0.2487 | 0.074 | 5 |
Li10Cr3Fe3(NiO8)2 (mp-775215) | 0.1886 | 0.094 | 5 |
Li10Cr2Fe3Co3O16 (mp-774310) | 0.2522 | 0.807 | 5 |
Li10Fe3Co3(NiO8)2 (mp-774318) | 0.2126 | 0.123 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV Cr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv V_pv Cr_pv O |
Final Energy/Atom-6.6043 eV |
Corrected Energy-249.9715 eV
Uncorrected energy = -224.5465 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.668 eV/atom x 2.0 atoms) = -3.3360 eV
Composition-based energy adjustment (-1.700 eV/atom x 3.0 atoms) = -5.1000 eV
Composition-based energy adjustment (-1.999 eV/atom x 3.0 atoms) = -5.9970 eV
Corrected energy = -249.9715 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)