Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.067 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.253 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNiPO4 |
Band Gap3.231 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 296.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 296.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 279.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 177.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 237.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 177.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 296.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 177.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 244.6 |
Ag (mp-124) | <1 1 1> | <1 1 0> | 119.0 |
BN (mp-984) | <0 0 1> | <0 0 1> | 296.5 |
BN (mp-984) | <1 1 0> | <1 1 0> | 238.1 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 296.5 |
LiNbO3 (mp-3731) | <1 0 1> | <1 1 0> | 238.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 296.5 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 279.6 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 296.5 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 296.5 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 296.5 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 244.6 |
SiC (mp-7631) | <1 1 1> | <1 1 0> | 238.1 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 237.2 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 237.2 |
GdScO3 (mp-5690) | <0 0 1> | <0 0 1> | 296.5 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 335.5 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 296.5 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 335.5 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 296.5 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 177.9 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 296.5 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 177.9 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 177.9 |
TbScO3 (mp-31119) | <1 1 0> | <0 1 0> | 335.5 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 0> | 210.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 296.5 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 105.1 |
InSb (mp-20012) | <1 0 0> | <0 1 0> | 279.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 238.1 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 279.6 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 118.6 |
NdGaO3 (mp-3196) | <0 0 1> | <0 1 0> | 335.5 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 177.9 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 177.9 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 279.6 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 279.6 |
SiC (mp-11714) | <1 0 1> | <0 1 1> | 163.0 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 105.1 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 177.9 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 223.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 59.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3(PO4)2 (mp-699908) | 0.5339 | 0.010 | 3 |
Co3(PO4)2 (mp-764887) | 0.5478 | 0.078 | 3 |
Na2Ge2O5 (mp-772811) | 0.5492 | 0.019 | 3 |
Cd3(PO4)2 (mp-680761) | 0.5530 | 0.000 | 3 |
Cd3(AsO4)2 (mp-13602) | 0.4001 | 0.000 | 3 |
LiCuPO4 (mp-758990) | 0.2001 | 0.072 | 4 |
LiCoPO4 (mp-772438) | 0.2052 | 0.194 | 4 |
LiCrPO4 (mp-761398) | 0.3575 | 0.045 | 4 |
LiFePO4 (mp-765950) | 0.2291 | 0.066 | 4 |
LiFePO4 (mp-761478) | 0.3700 | 0.057 | 4 |
LiMnPO4F (mp-762683) | 0.6142 | 0.211 | 5 |
Sr2AlCr2GaO7 (mvc-312) | 0.5808 | 0.186 | 5 |
Sr2AlGaCo2O7 (mvc-3397) | 0.6793 | 0.319 | 5 |
Li2PWO4F (mp-25728) | 0.6568 | 0.352 | 5 |
Na2LiCaVP2O9 (mp-763838) | 0.6620 | 0.111 | 6 |
Na2SrLiVP2O9 (mp-763837) | 0.6676 | 0.101 | 6 |
Na3LiMnBPO7 (mp-763842) | 0.7404 | 0.211 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv P O |
Final Energy/Atom-6.0556 eV |
Corrected Energy-378.9001 eV