Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.366 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.085 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiCoPO4 |
Band Gap2.271 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 185.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 268.3 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 165.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 268.3 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 288.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 309.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 371.5 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 206.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 268.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 61.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 350.8 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 20.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 82.5 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 103.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 330.2 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 268.3 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 165.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 371.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 268.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 330.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 82.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 268.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 82.5 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 61.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 227.0 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 185.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 309.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 103.2 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 268.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 144.5 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 268.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 350.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 268.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 144.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 144.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 185.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 268.3 |
BN (mp-984) | <1 0 1> | <0 0 1> | 309.6 |
BN (mp-984) | <1 1 1> | <0 0 1> | 268.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 268.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 61.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 61.9 |
Al (mp-134) | <1 0 0> | <0 0 1> | 330.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 82.5 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 185.7 |
LiGaO2 (mp-5854) | <1 1 1> | <0 0 1> | 268.3 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 330.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 330.2 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 268.3 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 144.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na2Cr2O5 (mp-1099683) | 0.6779 | 0.187 | 3 |
Sr2In2O5 (mp-22512) | 0.7016 | 0.029 | 3 |
Ca2Fe2O5 (mp-1076319) | 0.7265 | 0.047 | 3 |
Ca2Ga2O5 (mp-16433) | 0.6795 | 0.034 | 3 |
Ca2Al2O5 (mp-10444) | 0.7273 | 0.023 | 3 |
LiMnPO4 (mp-766155) | 0.3531 | 0.075 | 4 |
LiVPO4 (mp-850484) | 0.2154 | 0.053 | 4 |
LiNiPO4 (mp-768025) | 0.0732 | 0.056 | 4 |
Ca2MnAlO5 (mp-18907) | 0.6168 | 0.011 | 4 |
Ca2MnGaO5 (mp-25018) | 0.6100 | 0.003 | 4 |
K2Mn3V2(HO5)2 (mp-762295) | 0.7341 | 0.000 | 5 |
MnVHPbO5 (mp-762162) | 0.6685 | 0.000 | 5 |
NaZnMoHO5 (mp-540607) | 0.7264 | 0.007 | 5 |
VZnHPbO5 (mp-745150) | 0.6594 | 0.000 | 5 |
K3V2P2O8F3 (mp-1097033) | 0.6592 | 0.077 | 5 |
Explore more synthesis descriptions for materials of composition LiCoPO4.
Text computed by synthesisproject.org.
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCo: 3.32 eV |
PseudopotentialsVASP PAW: Li_sv Co P O |
Final Energy/Atom-6.5863 eV |
Corrected Energy-203.1493 eV
-203.1493 eV = -184.4167 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 7.4960 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)