Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.496 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLi3V2P4(HO8)2 + LiVPHO5 + VP + Li3PO4 + H2O |
Band Gap0.592 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [1] |
HallP 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 124.0 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 206.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 82.7 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 206.7 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 330.8 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 298.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 206.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 92.3 |
AlN (mp-661) | <1 0 1> | <1 -1 1> | 235.5 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 124.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 206.7 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 206.7 |
GaN (mp-804) | <1 1 0> | <1 -1 1> | 313.9 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 149.5 |
SiO2 (mp-6930) | <0 0 1> | <0 1 1> | 168.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 82.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 206.7 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 336.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 -1 1> | 313.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 165.4 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 92.3 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 276.8 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 206.7 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 92.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 336.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 1> | 92.3 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 276.8 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 124.0 |
CdS (mp-672) | <1 0 0> | <1 -1 0> | 206.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 186.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 289.4 |
CdS (mp-672) | <1 1 1> | <1 -1 0> | 275.6 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 206.7 |
LiF (mp-1138) | <1 1 0> | <1 1 1> | 92.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 289.4 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 289.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 330.8 |
YVO4 (mp-19133) | <1 0 1> | <1 1 1> | 276.8 |
YVO4 (mp-19133) | <1 1 0> | <1 1 0> | 250.5 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 257.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 206.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 250.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 336.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 149.5 |
BN (mp-984) | <1 0 0> | <0 0 1> | 261.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 224.2 |
BN (mp-984) | <1 1 0> | <0 0 1> | 261.5 |
BN (mp-984) | <1 1 1> | <0 1 0> | 248.1 |
LiNbO3 (mp-3731) | <1 1 1> | <0 0 1> | 261.5 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 124.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Fe3(PO4)4 (mp-705309) | 0.7211 | 0.127 | 3 |
Cr4P2O9 (mp-773396) | 0.6898 | 0.059 | 3 |
Cr5(PO4)4 (mp-540446) | 0.6779 | 0.007 | 3 |
Cr5(PO4)4 (mp-775246) | 0.6737 | 0.007 | 3 |
Fe3(PO4)4 (mp-31896) | 0.7143 | 0.127 | 3 |
LiNiPO4 (mp-766639) | 0.5630 | 0.089 | 4 |
Li3Sn3(PO4)4 (mp-758156) | 0.5930 | 0.071 | 4 |
Li3Sb3(PO4)4 (mp-758651) | 0.4909 | 0.064 | 4 |
ZnSn3P3O13 (mvc-10315) | 0.5773 | 0.161 | 4 |
Li3Sn3(PO4)4 (mp-757551) | 0.5504 | 0.059 | 4 |
LiVPHO5 (mp-767213) | 0.5155 | 0.000 | 5 |
LiSbPHO5 (mp-755185) | 0.4818 | 0.076 | 5 |
LiMnPHO5 (mp-769993) | 0.5310 | 0.000 | 5 |
Li2Cr2P4H3O16 (mp-763238) | 0.5488 | 0.056 | 5 |
Li4Cr2P4H3O16 (mp-774141) | 0.2300 | 0.033 | 5 |
Li2MnVP2(HO5)2 (mp-849523) | 0.4595 | 0.029 | 6 |
Li2MnVP2(HO5)2 (mp-776798) | 0.4515 | 0.038 | 6 |
Li2MnVP2(HO5)2 (mp-778728) | 0.4660 | 0.029 | 6 |
Li2MnVP2(HO5)2 (mp-777212) | 0.4564 | 0.030 | 6 |
Li2MnVP2(HO5)2 (mp-777091) | 0.4471 | 0.030 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Li_sv V_pv P H O |
Final Energy/Atom-6.6944 eV |
Corrected Energy-208.7370 eV
-208.7370 eV = -194.1364 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction) - 3.3640 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)